Failure analysis

Abrasive wear in alloy steel

Alloying elements form hard carbides in the steel, and those carbides abrade the tool. Wear appears as a polished land rather than a rough one, and it grows...

4 min read ·
Failure analysis

A change in sound as the first warning

A drill that starts to squeal is either rubbing or chattering, and the two sound different in a way that is learnable. Stopping at the squeal is cheaper than...

4 min read ·
Failure analysis

What chip shape tells you about feed

Long curls mean the feed is too light for the material to break the chip; short commas mean it is right; dust means the edge is rubbing. Chip shape is the ch...

4 min read ·
Failure analysis

Flank wear in carbon steel

Carbon steel is only mildly abrasive, so flank wear grows slowly and predictably. That makes it a good baseline: a tool that wears quickly here is running to...

4 min read ·
Failure analysis

Reading chip colour

Chip colour is the same temperature record as edge colour but read from the other side. Blue chips in steel mean the cut is running hot; silver chips mean it...

4 min read ·
Failure analysis

Chip form in carbon steel

Carbon steel produces a continuous chip at low feed and a broken chip at high feed. Which one appears decides whether the flute clears or packs, so feed is a...

4 min read ·
Failure analysis

Reading edge colour after a run

Colour on the edge is a temperature record: straw, brown, blue, then grey. The colour tells you what temperature the edge reached, which is more useful than...

3 min read ·
Failure analysis

Built-up edge in carbon steel

Carbon steel forms a built-up edge at low speed because the chip welds to the rake face before it can flow away. At higher speed the same steel cuts cleanly;...

4 min read ·
Failure analysis

A smeared rather than cut hole wall

Smearing means the material was displaced, not sheared. In ductile material that points to a light feed or a dull edge, and both make the next hole worse bec...

4 min read ·
Failure analysis

Springback in titanium holes

Titanium springs back after the tool passes, so the hole is smaller than the tool and the margin rubs on the way out. The measured hole size depends on the e...

4 min read ·
Failure analysis

Spiral marks on the hole wall

Regular spiral marks are a feed mark; irregular ones are chatter. Reading the spacing tells you which, and the spacing is set by feed per revolution or by a...

4 min read ·
Failure analysis

Chemical reaction with titanium

Titanium reacts with most coating materials at cutting temperature, so a coating that protects steel can dissolve in titanium. The countermeasure is to short...

4 min read ·
Failure analysis

Bell-mouth at hole entry

A widened entry means the tool was not guided when it started. A spot drill, a bushing or a shorter approach fixes the cause; a smaller drill does not.

4 min read ·
Failure analysis

Heat at the edge in titanium

Titanium keeps heat in a narrow zone next to the edge because its conductivity is low. The chip is thin and leaves fast, so the heat it removes is small and...

4 min read ·
Failure analysis

Taper in a deep hole

A deep hole that is smaller at the bottom than the top has either a worn tool, a deflecting tool or a buildup of chips that the margin is rubbing against. Me...

4 min read ·
Failure analysis

Galling on stainless hole walls

Galling is stainless transferred onto the tool and then torn back off the wall. It leaves a torn, picked surface and accelerates wear. Chlorinated coolant an...

4 min read ·
Failure analysis

Diagnosing an exit burr

An exit burr forms when the last material bends instead of shearing. Reduced feed at breakthrough, a backing plate or a different point angle each address a...

4 min read ·
Failure analysis

Heat concentration in stainless steel

Stainless conducts heat poorly, so the heat generated at the edge stays there. The chip carries away less than in carbon steel, and the tool has to survive a...

4 min read ·
Failure analysis

Diagnosing an entry burr

An entry burr is material pushed up rather than cut, which points to a dull edge or a point angle that is too blunt for the material. Increasing feed sometim...

5 min read ·
Failure analysis

Work hardening in stainless steel

Austenitic stainless hardens under the edge faster than the edge can cut through the hardened layer. Once the tool rubs instead of cutting, each pass makes t...

4 min read ·
Failure analysis

Why a small hole walks off centre

A slender tool deflects toward the softer side of the cut, so any asymmetry — grinding, runout, material variation — becomes a directional drift. The longer...

4 min read ·
Failure analysis

Smearing on aluminium hole walls

A smeared wall is material that was displaced rather than cut. It appears when the edge is dull, the feed is light, or the coating is chemically compatible w...

4 min read ·
Failure analysis

A hole that is in the wrong place

Position error comes from the approach, not from the drill: spot geometry, spindle position, or a tool that skidded on entry. A drill follows the hole that a...

4 min read ·
Failure analysis

Hole size drift in aluminium

An aluminium hole grows because the tool expands thermally and because the cut wall springs back less than in steel. The measured diameter therefore depends...

4 min read ·