ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

A smeared rather than cut hole wall

Smearing means the material was displaced, not sheared. In ductile material that points to a light feed or a dull edge, and both make the next hole worse bec...

4 min read 768 words Updated 2026-07-06
Cross-section of a drilled metal block showing the hole wall — A smeared rather than cut hole wall

DC326 carbide drills produce less smearing on hole walls due to their hardness range of 89–93 HRC, enhancing edge sharpness and durability. This reduces material displacement in ductile materials like aluminium at various cutting speeds (150–250 m/min), ensuring cleaner holes without work hardening the next pass.

The symptom as it appears

On the part, smearing appears as a rough, uncut surface on the hole wall instead of a smooth finish. Smearing occurs when feed rates are too light or cutting edges become dull, disrupting proper chip formation during drilling. Drill DC326 exhibits wear marks near its tip if used beyond optimal speeds and feeds for aluminium. These marks indicate material buildup and heat generation at the cutting edge.

Reduced cutting efficiency further leads to increased hole wall roughness. On the tool, a dulled cutting edge shows evidence of excessive friction against the workpiece material. This condition worsens with continued use, causing chips to compress rather than shear cleanly away. As a result, material on the hole walls becomes displaced instead of being cut smoothly and efficiently.

SpecificationValue
Point angle118 °
Carbide hardness89–93 HRC
Series diameter range0.04–3.17 mm

What can produce that symptom

Light feeds cause material displacement rather than cutting, which leads to smearing on hole walls. Smearing is more likely with dull edges due to increased friction and heat generation. Dull edges result from insufficient coolant application or prolonged use without maintenance. Work-hardening occurs when smeared material resists further cutting by the same tool conditions. Higher hardness of DC326 drills reduces edge wear, minimizing smearing during machining.

Smearing indicates ductile material displacement rather than clean shearing action. Light feeds exacerbate this issue by not applying enough force to initiate chip formation properly. Dull edges also contribute by failing to shear metal efficiently at optimal feed rates. Work-hardening from initial smearing makes subsequent holes even harder to cut cleanly. Adjusting feed rates and ensuring sharp tool edges help prevent further smearing incidents.

The order to check things

Begin by checking the feed rate settings against the recommended values for aluminium. Use lower rpm and higher feed rates to ensure proper chip formation. A feed of 50 mm/min at 25000 rpm may be too light for optimal cutting. Increasing to 100 mm/min can prevent material smearing. Verify that the DC326 drill is sharp before use; dull edges increase material deformation and work hardening.

Next, confirm that the coolant flow rate is adequate for chip evacuation and temperature control. Insufficient cooling may cause premature wear on the cutting edge. Check the geometry of the tool for any signs of damage or wear. Replace damaged drills to maintain edge integrity and sharpness. Adjusting these factors can significantly reduce smearing during drilling operations.

Confirming the cause before changing anything

To confirm smearing from light feeds or dull edges, inspect the hole wall surface for displaced material rather than cleanly cut chips. Rough surfaces indicate insufficient cutting forces that displace material instead of shearing it. For aluminum, use higher feed rates such as 100 mm/min to ensure proper chip formation and cutting action. Decrease spindle speed to 20000 rpm or lower to maintain optimal cutting conditions without overheating the tool. Check for a smooth finish after adjusting parameters; any remaining roughness suggests further adjustment is needed.

Ensure all inserts are sharp with an 118-degree point angle before running tests at recommended speeds and feeds. A dull edge increases friction, causing more material displacement rather than cutting. Smearing can also result from inconsistent chip thickness due to improper setup or worn tools. Confirm the geometry matches specifications; any deviation could lead to excessive heat and smearing issues. Adjustments should be incremental to prevent overcompensation that may cause other machining problems.

Frequently asked

Why is my hole wall smeared instead of cut?

A smeared hole wall indicates that the material was displaced rather than sheared, often due to too light a feed or a dull tool edge. This work-hardens the material, making subsequent holes worse.

What causes work hardening when drilling aluminium?

Light feeds and dull edges cause smearing in ductile materials like aluminium, which leads to work hardening which worsens with each hole drilled. Use proper cutting speeds and feeds to prevent this issue.

How do I avoid smeared holes when using DC326 carbide drills?

Ensure you use appropriate cutting parameters for the DC326 series: correct rpm (25000, 20000, or 16000), feed rates (50 to 1200 mm/min), and vc (150 to 250 m/min) to avoid smearing and work hardening.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index