ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Diagnosing an entry burr

An entry burr is material pushed up rather than cut, which points to a dull edge or a point angle that is too blunt for the material. Increasing feed sometim...

5 min read 909 words Updated 2026-06-06
Cross-section of a drilled metal block showing the hole wall — Diagnosing an entry burr

Carbide tools with an 118-degree point angle and hardness of 89–93 HRC minimize entry burrs by ensuring a sharp cutting edge on aluminum. These values prevent material from pushing up rather than shearing off cleanly, reducing waste during machining operations. Proper geometry and hardness allow the tool to engage the workpiece smoothly at high speeds like 150–250 m/min without creating an entry burr. Using DC326 series tools within a diameter range of 0.04 to 3.17 mm helps maintain consistent chip formation and surface finish, even with varying feed rates from 50 to 1200 mm/min. Ensuring sharp edges through regular maintenance prevents material buildup that causes entry burrs, enhancing tool life and part quality in aluminum machining.

The symptom as it appears

An entry burr appears as a raised ridge along the cut edge on aluminum parts. This burr forms when material pushes upwards rather than cuts cleanly away. The tool shows wear marks near the cutting edges where entry burrs occur frequently. These marks indicate that the cutting edge has become less sharp over time or use. A dull edge causes more friction and heat during cutting, exacerbating burr formation. When inspecting the part, a thin raised strip of aluminum can be seen at the start of the cut. This burr is often inconsistent in thickness across different sections of the workpiece.

The entry burr tends to reduce when using higher feed rates, as this helps the tool penetrate the surface more effectively. The DC326 series tools with an 118-degree point angle minimize initial contact area, reducing friction at entry points. A sharp cutting edge is crucial for clean cuts without pushing material upwards. When aluminum parts show signs of entry burrs, consider replacing or resharpening the tool to maintain optimal performance. Inspecting the DC326 tool reveals a gradual dulling of the edges near where contact occurs first. This indicates that the wear begins at the point angle and spreads along the cutting edge with continued use. Regular maintenance ensures consistent quality in machined parts by preventing entry burrs from forming.

SpecificationValue
Point angle118 °
Carbide hardness89–93 HRC
Series diameter range0.04–3.17 mm

What can produce that symptom

An entry burr forms when cutting forces push material upwards instead of shearing it cleanly off. This happens often with aluminum because its softness allows metal to deform easily. Using a dull tool increases likelihood of an entry burr as worn edges fail to cut efficiently. A point angle greater than 118 degrees also encourages burrs by reducing edge sharpness.

Optimal cutting speed for DC326 is between 150 and 250 m/min, outside this range raises risk. Increasing feed rate can sometimes mitigate entry burr formation by allowing the tool to penetrate faster. However, excessive feed may overheat the cutting edge causing premature wear. Always ensure proper coolant application when machining aluminum to prevent chip build-up.

The order to check things

Check for an entry burr by first examining if your tool is sharp enough or has a point angle too blunt, which is often the simplest and most cost-effective solution. A dull cutting edge or incorrect geometry can cause material to push up rather than cut smoothly. If that checks out, test whether increasing feed rates helps reduce the burr formation; higher feeds allow the cutter to engage below the surface more quickly in aluminum.

Remember, aluminum's softness means it deforms easily under pressure from a blunt tool. Always ensure your cutting speed and feed settings are within recommended ranges for optimal performance. Reviewing these basic factors first can often resolve entry burr issues without requiring further adjustments or equipment changes.

Confirming the cause before changing anything

To confirm an entry burr, inspect the tool edge for wear or a point angle that is too blunt for aluminum. A dull edge means material pushes upward instead of cutting smoothly away. A sharp tool with correct geometry reduces pushing forces on the workpiece surface. Ensure your DC326 tool has an 118-degree point angle for optimal performance. Measure cutting parameters such as rpm and feed rate to see if they fall within recommended values.

For aluminum, use rpm settings of 25000, 20000, or 16000 depending on the job demands. Check that your vc (cutting speed) is between 150 m/min and 250 m/min to avoid pushing material upwards. Adjust feed rate accordingly to prevent burr formation at entry points. Increasing feed can sometimes help by getting the cutting edge under the surface faster, reducing upward pressure on material. Always confirm tool sharpness before changing other parameters.

Frequently asked

What causes an entry burr when cutting aluminium?

An entry burr indicates a dull edge or point angle too blunt for the material being cut. For aluminium, ensure your tool has a sharp edge and a 118° point angle. Adjust feed rates to help the cutter engage properly.

How do I fix an entry burr on DC326 tools?

To address entry burrs with DC326 tools, check for dull edges or incorrect angles. Use appropriate cutting speeds like rpm ranges of 25000, 20000, and 16000, and feed rates of 50 to 1200 mm/min.

What are the recommended settings for DC326 tools in aluminium?

For optimal performance with DC326 on aluminium, use rpm between 25000 and 16000. Set feed rates from 50 to 1200 mm/min and maintain vc within 150 to 250 m/min range.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index