ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Diagnosing an exit burr

An exit burr forms when the last material bends instead of shearing. Reduced feed at breakthrough, a backing plate or a different point angle each address a...

4 min read 852 words Updated 2026-06-12
Cross-section of a drilled metal block showing the hole wall — Diagnosing an exit burr

A carbide drill with an 118-degree point angle and hardness between 89 and 93 HRC reduces exit burrs by improving chip control during breakthrough in aluminium workpieces. This precision minimizes material deformation at the exit, ensuring cleaner edges without compromising drilling efficiency. The DC326 series operates effectively across a range of spindle speeds from 16000 to 25000 rpm and feed rates up to 1200 mm/min. These parameters optimize cutting performance, reducing chip recutting and burr formation. A thinner drill diameter of 0.04 mm to 3.17 mm further enhances the tool's ability to manage chips and maintain sharpness during operation.

The symptom as it appears

An exit burr appears as a small raised edge on the drilled hole's exit side, measuring -0.003 mm thick. This burr forms when material deforms plastically rather than cutting cleanly at the end of the hole. Reduced feed rates near breakthrough can reduce this deformation by allowing more time for chip evacuation and cooling. A backing plate behind the workpiece supports the material during drilling, preventing it from flexing too much.

Adjusting to a different point angle, such as 118 degrees, changes how force is distributed at the cutting edge. This change helps control chip formation better but does not eliminate burr formation entirely. Smaller diameter drills, like those in the DC326 series, tend to produce less pronounced exit burrs due to their higher surface speed per tooth.

SpecificationValue
Point angle118 °
Carbide hardness89–93 HRC
Series diameter range0.04–3.17 mm

What can produce that symptom

An exit burr occurs when material deforms plastically rather than shearing at breakthrough. This deformation indicates insufficient feed rate or incorrect geometry settings. Higher spindle speeds reduce plastic deformation chances, but only within recommended limits. Exceeding these limits may cause tool wear or breakage issues instead of reducing the burr. Adjusting to 25000 rpm can help if current conditions produce excessive burrs.

Reduced feed rates at breakthrough also minimize exit burrs effectively. A backing plate placed behind the workpiece supports material stability during drilling. This support reduces plastic deformation and helps control chip formation better. Choosing a point angle of less than 118 degrees enhances cutting efficiency near the end. However, this change requires careful evaluation to avoid negative effects on hole quality elsewhere.

The order to check things

Start by reducing feed rates during breakthrough if burrs appear; slower feeds allow material to shear cleanly rather than deform plastically. A backing plate supports the workpiece, preventing material deformation at the exit side. Adjusting the point angle can also mitigate burr formation; a smaller angle applies more cutting force near the tip. Verify that your current rpm and feed match our recommended values for aluminium drilling: 25000 rpm, 50 mm/min or lower. If these changes do not resolve burrs, consider using DC326 drills specifically designed to minimize exit burs.

Next, check if your workpiece is properly clamped; inadequate support allows material deformation and burr formation at the exit side. Reduce feed rates in multiple stages approaching breakthrough to ensure consistent chip control and clean shearing of material. Ensure that your drill’s point angle matches the recommended 118 degrees for optimal performance against burrs. Compare your current drilling parameters against our guidelines: 20000 rpm, 100 mm/min for aluminium. If issues persist, consult our technical support for further assistance and troubleshooting tips.

Confirming the cause before changing anything

To confirm if insufficient feed causes exit burrs, measure material deformation at breakthrough carefully. Use a micrometer or similar tool for precise readings. If deformation exceeds -0.003 mm thickness, decrease feed rates gradually until clean cuts result. Adjusting feed rates to 50 mm/min initially often resolves issues without changing other parameters. A backing plate may be necessary if burrs persist despite reduced feed.

A 118-degree point angle geometry is effective in reducing exit burr formation by controlling chip flow dynamics. This angle directs chips away from the cutting edge, reducing friction and heat buildup at breakthrough. Testing confirms that carbide hardness ranging between 89 to 93 HRC remains unaffected during these adjustments. Always start with a slower feed rate before considering geometry changes for optimal results. If burrs still form, consider altering point angles incrementally while monitoring deformation closely.

Frequently asked

How do I fix an exit burr on carbide tools?

Reducing feed rate at breakthrough, adding a backing plate, or using a different point angle can help mitigate exit burrs. Adjust cutting parameters like rpm and feed rate based on material hardness and tool geometry.

What causes exit burrs in aluminum machining?

Exit burrs occur when the last chip bends rather than shears cleanly due to insufficient cutting force at breakthrough. This bending forms an unwanted ridge, often requiring parameter adjustment or different tooling.

Which DC326 series tool is right for aluminium without exit burr issues?

For aluminium, use a DC326 with an 118° point angle and ensure proper rpm settings such as 25000 to 16000 rpm. Adjust feed rates between 50 and 1200 mm/min according to material thickness for optimal results.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index