Failure analysis

A hole that measures small

An undersize hole is usually springback or thermal contraction after a hot cut, not a wrong tool. Measuring a warm part is the most common way to produce thi...

4 min read ·
Failure analysis

Chip welding in soft aluminium

Soft aluminium smears instead of shearing when the feed is too light. The chip is pressed onto the flute rather than lifted off it, and once the flute loads...

5 min read ·
Failure analysis

Failure analysis: Runout as an invisible cause of wear

When a tool runs out, one flute does all the work and wears faster. The hole is oversize and the edge chips on one side only. Because the tool itself is corr...

3 min read ·
Failure analysis

Holding a 3.175 mm shank in the wrong collet

An eighth-inch shank in a metric collet clamps on two points rather than around the circumference, which produces runout that no tool can absorb. The error i...

4 min read ·
Failure analysis

A hole that measures large

Oversize has several causes that look identical on a gauge: runout, an unbalanced edge, a worn margin, thermal growth or a workpiece that moved. The order to...

4 min read ·
Failure analysis

Built-up edge in aluminium

Aluminium welds to a sharp edge at low speed and high pressure. The weld grows until it changes the effective rake angle, then breaks away and takes carbide...

4 min read ·
Failure analysis

Continuing with a tool that has already worn

A worn drill still makes holes, which is why it gets used past its limit. The cost appears as a size drift across a batch that is attributed to the machine r...

3 min read ·
Failure analysis

A low-temperature coating in a hot cut

DLC and TiCN both have temperature ceilings below what a high-speed steel cut reaches. Above the ceiling the coating oxidises and the wear rate steps up rath...

4 min read ·
Failure analysis

Running full feed through breakthrough

At the instant the point exits, the load drops and the feed drive overshoots, so the tool lunges into the last material. That is where exit burrs and edge ch...

4 min read ·
Failure analysis

Failure analysis: Thermal cracking in interrupted cutting

Intermittent cutting heats and cools the edge repeatedly; the resulting cracks run perpendicular to the cutting edge. A tough substrate and a coating with a...

3 min read ·
Failure analysis

A peck cycle that pecks too often

Each retraction re-enters the hole and re-cuts chips that were already broken. A cycle that pecks more often than the chip needs adds rub time, heat and wear...

4 min read ·
Failure analysis

Failure analysis: Coating delamination on the cutting edge

A coating can flake off when the substrate deforms under load or when the interface is poorly prepared. The exposed substrate then wears quickly and the fail...

4 min read ·
Failure analysis

A step tool on a hole with one diameter

The step adds a diameter change, which adds a stress concentration and a second surface to control. On a plain hole it is a cost with no benefit.

4 min read ·
Failure analysis

Failure analysis: Poor hole wall finish from a carbide drill

A rough wall comes from chatter, chip re-cutting, a worn land or built-up edge. Each has a different appearance: chatter is regular, re-cutting is scored, a...

4 min read ·
Failure analysis

Failure analysis: Why a drilled hole comes out oversize

Oversize holes come from runout, an unbalanced tool, excess speed or a workpiece that moves. The drill diameter itself is only one term in the error stack, a...

3 min read ·
Failure analysis

Standard flute length in a deep hole

A flute shorter than the hole means chips have nowhere to go once the flutes are buried. The result is packing, heat and breakage, and it looks like a tool q...

4 min read ·
Failure analysis

Failure analysis: Entry burrs on drilled holes

An entry burr is material pushed up rather than cut, usually because the edge is dull or the point angle is wrong for the material. A sharper edge, a steeper...

4 min read ·
Failure analysis

Drilling an unsupported thin wall

The wall deflects under thrust, so the tool cuts less than it pushes. Supporting the exit side or reducing the point's thrust addresses the cause; increasing...

3 min read ·
Failure analysis

A nitride-coated tool in aluminium

The coating that protects a steel tool gives aluminium a surface to weld to, so the tool loads up and stops cutting. The fix is a different tool, not a diffe...

5 min read ·
Failure analysis

Failure analysis: Deflection of a long micro drill

A long tool of small diameter bends under side load, so the hole walks and the edge takes an uneven cut. Runout at the holder is magnified at the tip. Shorte...

4 min read ·
Failure analysis

Flood coolant in plastics

Plastics are cut cool by a sharp edge, and coolant mainly carries chips. Flood coolant can thermal-shock a hot weld line, so air blast is often the better an...

4 min read ·
Failure analysis

Failure analysis: Chip packing in deep small holes

Chips that cannot escape are re-cut, which raises torque and heat until the tool breaks. Peck cycles, adequate flute length and compressed air or coolant all...

4 min read ·
Failure analysis

Running stainless too slowly

A slow cut in stainless rubs, and rubbing hardens the surface faster than the edge can penetrate it. The instinct to slow down makes the problem worse rather...

4 min read ·
Failure analysis

Failure analysis: Burnt cutting edges from excessive speed

When speed is too high the edge loses hardness and the coating oxidises. The surface goes dark blue or brown and the tool fails early. This is a heat problem...