ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

A low-temperature coating in a hot cut

DLC and TiCN both have temperature ceilings below what a high-speed steel cut reaches. Above the ceiling the coating oxidises and the wear rate steps up rath...

4 min read 785 words Updated 2026-05-01
A snapped micro drill on a bench beside its broken tip — A low-temperature coating in a hot cut

The DC426 and DC836 carbide tools offer a black DLC or bronze TiCN coating, maintaining their hardness from HRC 89 to 93 even in high-speed steel cutting conditions. This range includes feed rates up to 270 mm/min and speeds up to 130 m/min. Above the typical temperature ceiling for these coatings, the DC426 and DC836 continue performing with minimal wear increase, extending tool life significantly. Their geometry, such as a 135-degree point angle, ensures stability across various cutting parameters from 20000 rpm down to 9000 rpm. This makes them suitable for applications that demand consistent performance despite thermal challenges.

What happens in the cut

The black DLC coating on DC426 and bronze TiCN coating on DC836 prevent oxidisation up to HRC 93 hardness range, resisting wear increase. At higher temperatures above their thermal limits, these coatings start to degrade rapidly. DLC remains stable in low-temperature environments but fails at around 500 degrees Celsius. TiCN performs similarly, with a degradation onset temperature also near 500 degrees Celsius. The geometry of both tools includes a 135-degree point angle for optimal cutting performance.

During high-speed steel cutting operations, the tool experiences peak temperatures that can exceed thermal limits of DLC and TiCN coatings. These conditions cause rapid wear due to coating oxidisation and loss of hardness properties. Maintaining stable feed rates and surface speeds helps manage heat generation during machining. Using coolant reduces temperature at the cutting edge but does not eliminate thermal issues entirely. Regular inspection is essential for monitoring tool condition and adjusting parameters as needed.

SpecificationValue
Point angle135 °
Carbide hardness89–93 HRC
Series diameter range0.04–3 mm

Why it looks like something else

At higher cutting speeds, above HRC 93, DLC and TiCN coatings oxidize more rapidly than expected. Oxidation causes a visible change in coating color from black or bronze to lighter shades. Lighter colors indicate increased wear because of oxidation, principal operators to misinterpret this as premature failure rather than normal high-temperature behavior. Prematurely replacing tools based on appearance wastes material and time. When using DC426 or DC836 at extreme conditions, maintaining consistent cutting parameters prevents unexpected discoloration.

Regular inspections help identify true wear patterns versus oxidation effects accurately. Adjusting feed rate or reducing spindle speed can mitigate early oxidation signs, extending tool life without compromising part quality. This adjustment ensures the coating operates within its designed temperature range for optimal performance. Understanding these visual cues enables better decision-making regarding tool maintenance and process optimization, enhancing overall efficiency in high-speed machining operations.

The real cause

At higher temperatures, above HRC 93 hardness range, DLC and TiCN coatings start to oxidize rapidly, which leads to a change in color from black or bronze to brown or grey. Oxidation weakens the chemical bonds within the coating layers, causing them to break down faster than at lower temperatures. This breakdown reduces wear resistance significantly. As temperature increases further, more iron particles deposit on the carbide surface, accelerating oxidization and which leads to rapid loss of coating integrity.

The deposited particles also cause abrasive wear. The geometry with a 135-degree point angle affects heat concentration during cutting. Higher angles reduce contact area, potentially raising local temperatures beyond the HRC 93 threshold faster. Reduced coating thickness from oxidation exposes more carbide surface, which leads to accelerated tool wear and reduced lifespan of DC426 and DC836 tools in high-speed operations.

The fix

The DC426 uses a diamond-like carbon coating that remains effective up to HRC 93 hardness level under various cutting conditions. When temperatures rise above this threshold, the DLC coating begins to oxidize, reducing its effectiveness against wear.

For higher-speed cuts where temperature exceeds HRC 93, switching to DC836 with TiCN coating is necessary for maintaining optimal performance and preventing rapid oxidation. The TiCN coating on DC836 performs well within a narrower range of cutting parameters than DLC but extends the usable temperature threshold slightly.

Frequently asked

How do DLC and TiCN coatings perform at high temperatures?

DLC and TiCN coatings have temperature limits below what high-speed steel reaches, typically around \(89-93 \, \text{HRC}\). Above these temperatures, they oxidise, which leads to faster wear.

What is the point angle for carbide tools in this article?

The geometry values include a \(135^\circ\) point angle. This configuration helps manage heat and reduce cutting forces during machining operations.

Can you provide cutting data for alloy use with DC426 or DC836 series?

For DC426 and DC836, recommended cutting speeds range from 70 to 130 m/min at \(20000 \, \text{rpm}\), \(13000 \, \text{rpm}\), and \(9000 \, \text{rpm}\) with feeds of 40 mm/min, 60 mm/min, 100 mm/min, and 270 mm/min.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index