ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Failure analysis: Thermal cracking in interrupted cutting

Intermittent cutting heats and cools the edge repeatedly; the resulting cracks run perpendicular to the cutting edge. A tough substrate and a coating with a...

3 min read 673 words Updated 2026-04-24
Close-up of a worn carbide drill edge with a visible wear land — Failure analysis: Thermal cracking in interrupted cutting

Thermal cracking occurs when repeated heating and cooling stress the carbide edge, causing perpendicular cracks. Tough substrates with high thermal conductivity from 89 to 93 HRC reduce crack propagation. Cycles of rapid temperature change require a coating with expansion rate matching the substrate’s, preventing delamination. A point angle of 140 degrees distributes heat more evenly during intermittent cutting. At speeds up to 270 mm/min feed and 130 m/min cutting velocity, this setup minimizes thermal stress on the tool edge.

The symptom as it appears

The part surface shows irregular wear patterns with fine cracks near the cutting edge. These cracks are perpendicular to the direction of cut, often forming a network.

Tool wear features similar lines along the flute where the insert engages the workpiece repeatedly. The cutting edge displays small, branched fractures that propagate inward from the tip.

What can produce that symptom

High cutting speeds or feeds that exceed recommended values exacerbate thermal stresses on carbide edges, which leads to cracks perpendicular to the cutting direction. Using a substrate with hardness below 89 HRC and thermal conductivity in the range of 80–100 W/(m·K) helps resist thermal cracking better than harder materials might at high speeds. Interrupted cuts create intense localized heat followed by rapid cooling, which causes thermal stresses that can initiate cracks if not managed properly.

A point angle of 140 degrees provides a large surface area for heat dissipation during interrupted cutting operations but does little to prevent crack propagation once initiated. Reducing the number of interruptions per minute decreases stress cycles on the tool edge, slowing down crack formation and extending tool life significantly in applications with frequent stops.

The order to check things

Check the cutting parameters first for speeds and feeds within recommended ranges. Exceeding these can intensify thermal stresses, causing cracks perpendicular to the edge. Next, inspect the tool geometry closely; a point angle of 140 degrees helps distribute heat evenly. Ensure that your tools match this specification exactly for optimal performance. Verify that the workpiece material does not generate excessive heat during cutting operations.

This exacerbates existing thermal issues and accelerates crack formation significantly. Assess the condition of the coolant supply to ensure it reaches all critical areas effectively. Insufficient cooling increases localized heating, promoting rapid wear and cracking at the edges. Lastly, review the surface finish requirements carefully; smoother finishes demand finer cuts that reduce heat generation. Adjust cutting parameters accordingly to minimize thermal stress on the tool edge.

Confirming the cause before changing anything

To confirm thermal cracking, inspect for perpendicular cracks on the cutting edge under a microscope. Cracks appear as fine lines near the tool tip and spread along the direction of cooling cycles. Compare actual cutting parameters to recommended values provided by the manufacturer. Excessively high speeds or feeds can intensify thermal stress, promoting crack formation prematurely. Adjusting these settings closer to guidelines helps mitigate excessive heating during interrupted cuts.

Softening the cutting cycle reduces the frequency and severity of temperature fluctuations. Implementing a more consistent feed rate and adjusting speed for smoother operation is critical. A stable process minimizes sudden heat changes that can propagate thermal cracks quickly. Choosing an appropriate coolant flow also plays a vital role in controlling edge temperatures. Maintaining these conditions ensures better tool life by preventing premature crack propagation.

Frequently asked

How do I prevent thermal cracking when interrupted cutting?

Reduce cycle time and increase coolant flow to minimise heating-cooling cycles on the carbide edge. Use tools with tough substrates and coatings that match thermal expansion rates.

What causes thermal cracks in carbide tools during interrupted cutting?

Thermal cracks form due to rapid temperature changes at the cutting edge. As the tool heats up and cools down repeatedly, perpendicular cracks develop along the edge, weakening it over time.

Can changing feed rate stop thermal cracking?

Adjusting feed rates can help but does not guarantee prevention. Faster feeds may reduce heat build-up by shortening contact times, yet optimal settings depend on material hardness and cutting conditions.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index