ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Springback in titanium holes

Titanium springs back after the tool passes, so the hole is smaller than the tool and the margin rubs on the way out. The measured hole size depends on the e...

4 min read 787 words Updated 2026-07-03
Brushed stainless steel block with drilled holes — Springback in titanium holes

DC426L tools with an 89–93 HRC hardness cut titanium with minimal margin wear due to their sharp edges and durable coating. Their 135° point angle minimizes cutting forces, reducing deformation during springback. At speeds of 3000 to 10000 rpm and feeds of 20 to 80 mm/min, these tools maintain hole accuracy better than softer alternatives. This precision is critical for titanium parts where elastic recovery can distort the finished diameter significantly. By minimizing margin contact, DC426L ensures consistent quality despite material variability.

The mechanism

The tool's sharp edge cuts through titanium with minimal wear on the margin. As it exits, the hole is slightly smaller than the tool diameter due to material springback. This springback effect depends on titanium’s high elastic recovery properties after deformation. The exit clearance becomes critical as the margin can rub against the workpiece surface during withdrawal. Increasing feed rate or reducing cutting speed can mitigate this issue but may affect tool life and surface finish.

The 135° point angle of the DC426L ensures a concentrated chip removal path, minimizing built-up edge formation. The carbide hardness from 89 to 93 HRC contributes to enduring wear resistance under high-stress conditions. Durability allows for consistent hole dimensions across multiple operations. However, operators must monitor tool condition and adjust parameters accordingly for optimal performance. Proper adjustment of these settings helps maintain the required tolerance in titanium workpieces.

SpecificationValue
Point angle135 °
Carbide hardness89–93 HRC
Series diameter range0.04–3 mm

The conditions that produce it

High cutting speeds between 40 m/min and 80 m/min increase springback because they reduce friction and heat buildup, allowing titanium to recover more rapidly. Springback occurs less when using lower feed rates of 20 mm/min or 40 mm/min rather than higher rates like 80 mm/min. Higher rpm settings also contribute significantly to increased springback effects. Lower speeds between 3000 rpm and 6000 rpm minimize springback compared to faster speeds of 10000 rpm, as slower rotations allow material time to recover elastically after cutting passes through.

The geometry with a 135-degree point angle ensures stability but also affects the amount of springback by influencing how much force is applied during exit from the hole. Higher feed rates above 40 mm/min accelerate wear on the tool's margin, increasing springback issues. Using lower cutting speeds and moderate feed rates helps maintain hole size accuracy in titanium, reducing the impact of elastic recovery after machining operations are completed.

How to recognise it on the tool

Springback appears as a smaller hole than expected when cutting titanium. The margin of DC426L tools shows wear at entry and exit points. Tool marks on the part surface indicate where metal rubbed against the tool edge. These marks can be mistaken for chatter or poor alignment issues. The sharp 135° point angle cuts cleanly but leaves a small clearance gap post-cutting.

This results in springback, making holes smaller than intended after cutting. Operators should inspect for consistent wear patterns on both entry and exit sides of the tool margin. Irregular patterns might suggest other problems unrelated to springback. Understanding these signs helps differentiate between typical springback effects and potential machining errors or material inconsistencies.

What actually removes the cause

Springback occurs because titanium's elastic recovery exceeds the tool diameter after cutting. High hardness carbide tools wear less, ensuring consistent hole size during exit. DC426L has a 135° point angle that reduces friction and minimizes margin wear. Lower speeds below 40 m/min increase friction, hindering springback but causing more heat and wear. Higher speeds above 80 m/min reduce friction too much, allowing titanium to recover excessively.

A common fix involves reducing cutting speed or increasing tool diameter. This approach can reduce visible wear on the tool margin but does not address underlying material recovery issues. Adjusting feed rates alone cannot overcome springback at extreme speeds. Instead, using optimized geometry and hardness minimizes margin contact and friction losses during cutting operations. Such tools maintain hole accuracy across a wider range of titanium alloys and cutting conditions.

Frequently asked

How does springback affect titanium hole sizes?

Springback in titanium causes holes to shrink after cutting, making them smaller than intended and causing margin rub as tools exit. This effect varies based on alloy elasticity.

What is the ideal point angle for drilling titanium?

A 135° point angle works well for drilling titanium due to its ability to manage springback and maintain hole accuracy despite material deformation.

Which DC426L part number should I use for titanium drilling?

For titanium, use DC426L with a hardness range of 89–93 HRC. This series handles the high elasticity and springback properties of titanium effectively.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index