ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Reading edge colour after a run

Colour on the edge is a temperature record: straw, brown, blue, then grey. The colour tells you what temperature the edge reached, which is more useful than...

3 min read 669 words Updated 2026-07-12
Close-up of a worn carbide drill edge with a visible wear land — Reading edge colour after a run

Edge colour after cutting shows temperature exposure, indicating tool performance and potential wear issues. Straw indicates lower temperatures; brown means hotter but still within limits. Blue signals severe overheating near failure point; grey marks catastrophic failure. Understanding these colours helps predict tool life and optimise machining parameters accordingly. This knowledge prevents costly tool breakages and improves overall process efficiency.

The symptom as it appears

After a cutting run, the edge of DC836 appears with distinct colour bands reflecting temperature exposure during operation. These bands typically start from the tip towards the shank, indicating where temperatures were highest.

Straw-coloured bands suggest normal operating conditions with lower temperatures. Brown bands appear at intermediate temperatures and indicate moderate wear or higher speeds. Blue areas show extreme heat, often near failure points. Grey marks signal severe overheating and imminent tool breakage.

SpecificationValue
Point angle118 °
Carbide hardness89–93 HRC
Series diameter range0.1–14 mm

What can produce that symptom

High cutting speeds and feeds above recommended values cause excessive heat on DC836's edge, showing up as darker bands post-run. If the rpm is set too high for the material hardness, the temperature spike reaches blue or grey levels quickly. Proper selection ensures longevity. Feeds that are too light result in higher localized temperatures at the cutting edge, often which leads to discoloration along the edge after use. Correct feed rates distribute heat more evenly across the tool surface.

Incorrect depth of cut can also induce high temperatures, pushing the edge beyond its temperature tolerance and causing rapid discolouration. Adjusting ap within specified limits reduces this risk significantly. Combining improper settings with hard materials intensifies thermal stress, further accelerating wear and tear on DC836's cutting edges. Ensuring optimal parameters for each operation preserves tool integrity.

The order to check things

After a run, inspect edge colour on DC836 first with a magnifying glass or microscope for detailed analysis. Start by checking the outermost areas where temperatures typically peak. Begin with lower magnification to spot broad temperature bands quickly. Higher magnification reveals finer details about specific cutting conditions experienced. Cheapest inspection methods come first: naked eye, then hand lens at minimal cost.

Advanced tools like microscopes are last due to higher expense and complexity. Always document observed colours and their locations on the edge for future reference and comparison. This practice helps in identifying trends over multiple runs efficiently. Compare current run's colour bands with previous ones under similar conditions. Noting changes aids in adjusting cutting parameters proactively to prevent tool failure.

Confirming the cause before changing anything

Before changing any cutting parameters, check edge colour under a magnifying glass or microscope for signs of overheating. Compare the colours to known standards: straw indicates moderate heat, brown signifies higher temperatures, blue marks severe heating, grey shows extreme conditions. If the edge appears with dark bands, especially grey, reduce the speed and feed rates immediately to prevent further damage. Darker bands near the cutting tip suggest excessive friction or insufficient cooling fluid application.

Lighter colours farther from the cutting area indicate better temperature control at those sections of the tool. Adjusting coolant flow can also help manage heat in critical areas effectively. After modifying parameters, re-run a test and inspect edge colour again to confirm improvements before full production starts.

Frequently asked

What does the edge color mean on carbide tools after cutting?

The colour of your carbide tool's edge indicates how hot it got during use: straw shows low temp, brown is higher, blue means very high, and grey signals overheating.

How hard is DC836 carbide?

DC836 has a hardness range between 89 to 93 HRC, making it extremely durable for various cutting operations without losing edge integrity.

What rpm should I use with DC836 tools?

Use DC836 at speeds up to 20000 rpm for optimal performance. Adjust to 13000 rpm or 9000 rpm based on material hardness and desired finish quality.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index