24 articles on this page
Tool design

Point thinning and thrust reduction

Thinning removes web material behind the chisel edge. It reduces thrust sharply and is the single largest change available to a small drill in hard material,...

3 min read ·
Coatings

AlTiN coating for alloy steel

At high cutting speed the edge reaches a temperature where TiN and TiCN oxidise. AlTiN keeps its hardness further up the temperature scale, which is the only...

4 min read ·
Cutting parameters

Through-tool coolant and the depth it unlocks

Internal coolant delivers fluid to the point rather than to the flute, which is what makes holes deeper than a few diameters possible at all. The tooling cos...

4 min read ·
Series notes

DC326: when it is the wrong tool

The uncoated series is the right default for soft and non-ferrous work and the wrong one for abrasive steel, where the absence of a wear layer shortens life...

4 min read ·
Failure analysis

Notch wear at the depth of cut

Notch wear appears where the edge crosses the workpiece surface, because that line is where the edge rubs on already-cut material. It deepens until the corne...

4 min read ·
Tool design

Length-to-diameter ratio as a design limit

Stiffness falls with the cube of length, so a tool at ten diameters deep is a different problem from the same tool at three. The ratio, not the diameter, dec...

3 min read ·
Cutting parameters

Air blast versus flood in micro holes

Air removes chips without thermal shock and without the cost of fluid handling. Flood cools better but cannot reach the edge at depth. In graphite and lamina...

4 min read ·
Precision & tolerance

Coating thickness and the finished diameter

A coating adds to the diameter as well as to the surface, so a coated tool is ground undersize to finish on nominal. A shop that mixes coated and uncoated to...

4 min read ·
Failure analysis

Abrasive wear in alloy steel

Alloying elements form hard carbides in the steel, and those carbides abrade the tool. Wear appears as a polished land rather than a rough one, and it grows...

4 min read ·
Coatings

AlTiN coating for nickel-based alloys

Nickel alloys hold heat at the edge and attack the tool chemically. AlTiN's hot hardness and oxide layer are the closest thing to protection, but the notch t...

4 min read ·
Failure analysis

A change in sound as the first warning

A drill that starts to squeal is either rubbing or chattering, and the two sound different in a way that is learnable. Stopping at the squeal is cheaper than...

4 min read ·
Cutting parameters

Coolant concentration and what it actually does

Coolant lubricates, cools and flushes, and concentration sets the balance. Too lean and stainless galls; too rich and the fluid foams and stops flushing, whi...

4 min read ·
Precision & tolerance

Accepting a size drift across a tool's life

A drill that starts at nominal and finishes at the top of tolerance has used the whole band, so the next regrind has nowhere to go. Acceptance criteria shoul...

4 min read ·
Cutting parameters

Speeds and feeds for 10 to 14 mm drilling

At this diameter the cutting speed in steel is low enough that the spindle may not reach the recommended rpm. Feed per revolution then has to be reduced to k...

4 min read ·
Failure analysis

What chip shape tells you about feed

Long curls mean the feed is too light for the material to break the chip; short commas mean it is right; dust means the edge is rubbing. Chip shape is the ch...

4 min read ·
Tool design

Back taper on a deep-hole drill

Back taper reduces the diameter behind the point so the tool does not rub along a deep hole. Without it, friction rises with depth until the tool stalls or b...

4 min read ·
Tool design

Drilling 0.2 mm holes in carbon steel

At 0.20 mm the flute just has room to carry a chip, which makes evacuation possible for the first time in the micro range. Carbon steel is the forgiving case...

4 min read ·
Failure analysis

Flank wear in carbon steel

Carbon steel is only mildly abrasive, so flank wear grows slowly and predictably. That makes it a good baseline: a tool that wears quickly here is running to...

4 min read ·
Coatings

AlTiN coating for titanium alloys

AlTiN forms an aluminium oxide layer at temperature that slows the chemical reaction between the tool and titanium. It buys time, not immunity: the speed sti...

4 min read ·
Series notes

DC426 versus DC836 when both fit

Their diameter ranges overlap around 0.1 to 3 mm. The black coating and the bronze coating fail differently: one at the edge, one across the flank, which cha...

3 min read ·
Failure analysis

Reading chip colour

Chip colour is the same temperature record as edge colour but read from the other side. Blue chips in steel mean the cut is running hot; silver chips mean it...

4 min read ·
Tool design

Margin width and hole wall contact

The margin is the part of the tool that touches the wall. A wide margin guides the drill and rubs; a narrow one cuts freer and wanders. Which is better depen...

4 min read ·
Cutting parameters

Speeds and feeds for 6 to 10 mm drilling

Feed per revolution is now limited by the machine's thrust and by the workpiece fixture. At this size an unstable setup shows up as chatter marks rather than...

4 min read ·
Precision & tolerance

When to inspect a drilled hole

Before deburring, after cleaning, at temperature: each stage changes the number. The inspection point has to be fixed in the procedure or the measurements wi...