Application notes, process notes and product notes from the TONNY engineering team. Each article ties a catalogue geometry to the operation it performs and the failures it prevents.
Galling is stainless transferred onto the tool and then torn back off the wall. It leaves a torn, picked surface and accelerates wear. Chlorinated coolant an...
Ra on a drilled wall is set by feed marks and by smearing, so the specification has to say whether it applies along the axis or around the circumference. The...
At 0.10 mm the edge radius is still a large part of the cross-section, so the cut is closer to extrusion than to shearing and the surface is formed rather th...
Speed and feed tables for this band are reliable enough to use directly. The variable that most affects the result is not the number but the consistency with...
An exit burr forms when the last material bends instead of shearing. Reduced feed at breakthrough, a backing plate or a different point angle each address a...
140 degrees pushes further into the hard-material range: less thrust per unit edge length, more point length, and a weaker point that has to be supported by...
Pulling out too fast drags the margin across the wall and can break the edge off. Pulling out too slowly re-cuts chips that were already cleared. The rate sh...
Brass is drilled at moderate speed with a short chip, so neither wear nor heat is the limit. An uncoated edge avoids the adhesion that a nitride coating can...
At 0.10 mm the edge radius is still a large part of the cross-section, so the cut is closer to extrusion than to shearing and the surface is formed rather th...
Stainless conducts heat poorly, so the heat generated at the edge stays there. The chip carries away less than in carbon steel, and the tool has to survive a...
Position error is the sum of machine position, spindle runout, spot accuracy and drill deflection. The drill contributes the last term only, and it is usuall...
Both are TiN-coated left-hand tools. The difference is the diameter range and the SKU count, which reflects how many diameter and length combinations each fo...
135 degrees is the stainless and hard-material point. The flatter angle spreads thrust over a longer edge and reduces the work-hardening that a blunter point...
Cutting speed now matters thermally: at 0.5 mm the surface speed at 20,000 rpm is high enough that a coating with hot hardness changes tool life. Feed can be...
In ceramics the tool fails by edge chipping, and a coating does not prevent a chip. The uncoated grade is selected for toughness and for the ability to hold...
An entry burr is material pushed up rather than cut, which points to a dull edge or a point angle that is too blunt for the material. Increasing feed sometim...
A short dwell lets the tool finish the cone before retracting, which cleans the bottom. Too long a dwell rubs, work-hardens the point and burns the edge, so...
Austenitic stainless hardens under the edge faster than the edge can cut through the hardened layer. Once the tool rubs instead of cutting, each pass makes t...
At 0.10 mm the edge radius is still a large part of the cross-section, so the cut is closer to extrusion than to shearing and the surface is formed rather th...
DC836 is bronze-coated and reaches 14 mm; DC826 is uncoated and general purpose. Where the hole is small enough for both, the coating decides, and the bronze...
130 degrees appears where delamination and entry quality matter: PCB laminate and composite stacks. The steeper point shears the top layer before pushing it,...
Feed per tooth at this diameter can be set from the general micro range, and the limit becomes chip load per flute rather than tool strength. Higher feed usu...
A hole can be exactly on diameter and out of round, because a two-flute tool cuts an approximate circle from two arcs. The diameter gauge will not show it an...
A slender tool deflects toward the softer side of the cut, so any asymmetry — grinding, runout, material variation — becomes a directional drift. The longer...
Articles are written against the production catalogue. Dimensions and part numbers referenced in the text resolve to the same records used by the series and diameter pages.