A short dwell at the bottom of a hole ensures clean edges without excessive heat or wear. This avoids work-hardening and edge burning, maintaining sharpness for subsequent cuts. A 135-degree point angle efficiently removes material with minimal friction. Hardness between 89–93 HRC resists deformation during rapid retraction. Optimal dwell balances flat bottom surfaces with reduced risk of carbide deterioration.
The variable and the range it can take
The dwell time is a crucial variable for finishing holes cleanly. It should be long enough to complete cutting but short to prevent heat build-up and edge damage. A longer dwell can work-harden the material, increasing friction at the tool point. This extra wear affects the carbide's hardness range of 89–93 HRC over time. Shorter dwell reduces contact time, minimizing thermal stress on the cutting edge.
Dwell duration is expressed in milliseconds and ranges from a few to dozens based on hole size and material type. For instance, stainless steel requires faster speeds at 15000 rpm compared to common steels at 7000 rpm or 5000 rpm. Feed rates also vary between materials: stainless uses 30 mm/min, while general steel can use up to 150 mm/min. Depth of cut (ap) and chip thickness per tooth (fz) must match the material's hardness for optimal performance. Adjusting these parameters ensures consistent hole quality without damaging the cutting edge.
| Specification | Value |
|---|---|
| Point angle | 135 ° |
| Carbide hardness | 89–93 HRC |
| Series diameter range | 0.04–3 mm |
What it changes in the cut
A longer dwell increases cutting force on the tool edge at the hole bottom. This raises temperatures sharply due to friction between the material and carbide. Higher temperatures soften the HRC 89-93 hard carbide coating quickly. Softened steel cuts poorly, which leads to more wear and potential breakage during drilling. Reducing dwell time lowers cutting forces, keeping temperatures within safe limits for tool integrity.
Lower temperatures prevent work-hardening of stainless steel in critical areas. Work-hardening makes the material tougher to cut as it progresses through the hole. This increases the risk of chipping or cracking if the force is not managed properly. A shorter dwell also affects chip formation by reducing frictional heat at the cutting edge. Smaller, thinner chips form more easily when less heat degrades lubrication and cooling effectiveness.
Where the limit comes from
Carbide's high hardness range from 89 to 93 HRC makes it wear-resistant but also brittle at extreme temperatures.
Excessive heat during long dwells can lower the tool’s hardness temporarily, increasing edge wear and risk of chipping.
Setting it in practice
Excessive heat during long dwells can damage carbide edges, reducing tool life significantly. Set initial dwell times between 0.5 and 1 second for a balanced approach. Start with stainless steel at 7000 rpm and 45 mm/min feed rate. Adjust dwell duration based on observed edge wear and hole bottom finish quality. Monitor cutting force to detect early signs of overheating or excessive friction.
For common materials, begin testing at 5000 rpm and a slower feed of 30 mm/min. Use the general fz values for optimal chip control and surface finish. Observe how changes in dwell affect edge sharpness and hole flatness. Reduce dwell if you notice rough edges or signs of overheating. Ensure consistent tool life by maintaining proper cutting parameters during operations.
Frequently asked
What is the recommended dwell time for carbide tools when drilling stainless steel?
A short dwell allows finishing the cone before retraction, cleaning the hole bottom. Too long can rub and work-harden the point, burning the edge. Balance flatness and heat.
How do I avoid overheating with DC426 drills in stainless steel?
Use a shorter dwell time to prevent excessive friction at the hole bottom. Adjust feed rate and speed within specifications: rpm 15000-7000 for optimal results, avoiding tool wear and surface damage.
What is the right point angle for drilling stainless steel with DC426 tools?
A 135° point angle works well for most stainless steels. It balances cutting efficiency and chip evacuation, reducing heat buildup during drilling operations.