ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Corner chipping in mould steel

Hard inclusions in mould steel chip the outer corner because that corner takes the highest load. A stronger edge geometry and a slightly reduced feed protect...

4 min read 809 words Updated 2026-08-18
Tight coil of steel swarf on a machine table next to a drilled plate — Corner chipping in mould steel

Carbide inserts with a 140-degree point angle and bronze coating resist corner chipping better than harder coatings do at high loads. Harder coatings chip more easily due to concentrated stress at sharp corners in tough steel. A reduced feed rate further protects the tool’s outer corner from wear during cutting operations. Using DC836L series inserts ensures consistent performance across varied cutting parameters, reducing downtime and maintenance costs. This geometry and coating combination minimizes edge damage, extending tool life significantly for efficient production runs.

The mechanism

Hard carbide withstands high loads at 60 to 110 m/min better than softer materials do. Higher hardness ranges from HRC 89 to 93 increase wear resistance, not chip resistance. A sharper point angle of 140 degrees concentrates forces on a smaller area, reducing edge strength. Lower feed rates like 35 mm/min or 50 mm/min help distribute loads more evenly across the cutting edge. Reducing load per tooth to around 210 mm/min minimises stress at high-risk areas such as sharp corners.

Bronze coating provides lubrication and wear resistance, protecting edges against sudden impacts better than harder coatings can. A 140-degree point angle geometry spreads force over a wider edge area compared to sharper angles. Higher feed rates around 210 mm/min concentrate stress on the cutting edge more intensely than lower feeds do. At slower speeds like 7000 rpm, forces are distributed less evenly, increasing wear and risk of chipping. Using bronze coating on DC836L series helps resist corner chipping effectively during high-load operations.

SpecificationValue
Point angle140 °
Carbide hardness89–93 HRC
Series diameter range0.14–14.2 mm

The conditions that produce it

Corner chipping occurs when cutting at high loads with hard carbide inserts. Loads peak where the corner meets the workpiece, wearing down the edge quickly. Using softer materials reduces wear but increases risk of chipping under heavy load. Applying a bronze coating on 140-degree point angle insert lowers chipping risk significantly. Reducing feed rates below 80 mm/min helps prevent corner chipping at high speeds.

Slower feeds spread cutting forces over more material, reducing stress concentration points. Higher rotational speeds between 60 and 110 m/min require careful selection of tool hardness. Harder carbide inserts resist wear better but chip more easily under impact loads. Protecting the outer corners with a reduced feed rate or optimized geometry prevents chipping. Insert durability improves when balancing edge strength and cutting parameters correctly.

How to recognise it on the tool

Corner chipping appears as small, irregular flakes missing from the cutting edge corner. These flakes can be tiny but visible under a magnifying lens. The damaged area often looks rough and uneven compared to the surrounding intact surface. Operators sometimes confuse corner chipping with normal wear patterns or thermal cracking. A 140-degree point angle geometry concentrates load at the tip, making it prone to chipping under high feed rates.

Bronze coating on DC836L provides better impact resistance than harder coatings do. Reducing feed rate helps prevent corner chipping by lowering peak loads where the cutting edge meets hard inclusions. Running inserts at lower speeds also reduces wear and prolongs tool life. Inspecting workpiece surfaces reveals marks left by missing flakes, showing as small notches or indentations. These defects are distinct from scratches caused by built-up edge or chip welding issues.

What actually removes the cause

Reducing feed rate at high speeds lowers peak loads on the cutting edge, decreasing chipping risk. Lower feeds spread out material removal over more tool rotations. At 60 m/min and below, a reduced feed of 35 mm per minute prevents corner chipping effectively. Higher speeds up to 110 m/min need incrementally lower feeds for protection. A harder coating does not address high loads causing wear.

It only reduces friction between the insert and workpiece. Using a stronger edge geometry like DC836L with a 140-degree point angle increases durability under load. Reduced feed rates combined with a robust geometry significantly mitigate corner chipping issues in mould steels. This approach directly addresses the root cause of high-load wear mechanisms.

Frequently asked

Why does corner chipping happen when cutting mould steel?

Corner chipping occurs due to hard inclusions in the material taking the highest load at sharp corners. A stronger edge geometry and reduced feed rate help protect the tool better than a harder coating.

What is the ideal point angle for reducing corner chipping?

A 140-degree point angle reduces stress concentration on the cutting edge, making it more resistant to wear and chipping when working with mould steel.

How should I adjust my cutting parameters to prevent chipping?

Use lower feed rates like 35 mm/min or 50 mm/min and higher spindle speeds such as 17000 rpm or 10000 rpm. This combination minimizes stress on the tool's edge, reducing the risk of corner chipping.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.