A stronger edge preparation on DC836L prevents chipping at the outer corner under harsh conditions. This feature is crucial because hard inclusions or interrupted cuts cause rapid wear and failure here. Edge durability increases by reducing stress concentration at sharp points, extending tool life significantly. Hardness levels of 89–93 HRC combined with a 118° point angle enhance resilience against impact forces. These improvements allow for stable cutting even when feed rates are high or speeds fluctuate widely.
The symptom as it appears
On parts processed with DC836L carbide tools, chipping appears at the outer corner first due to high stress concentration. This damage is visible as a jagged break along the cutting edge near the point angle of 118 degrees. Chipped corners reduce tool life and degrade part quality noticeably. When inspecting the tool after use, operators will find missing material flakes on the side closest to the workpiece entry point.
This indicates frequent impacts from hard inclusions or interrupted cuts. The bronze coating applied to DC836L resists wear but does not prevent chipping as effectively as a stronger edge preparation can. Operators should observe closely for any signs of premature wear or damage at the outer corner during tool use, especially under high feed rates and cutting speeds.
| Specification | Value |
|---|---|
| Point angle | 118 ° |
| Carbide hardness | 89–93 HRC |
| Series diameter range | 0.14–14.2 mm |
What can produce that symptom
Chipping at the outer corner often occurs when cutting through materials with hard inclusions that can abruptly increase tool load. DC836L carbide tools handle interruptions well due to their 89–93 HRC hardness range, but edge wear still happens under extreme conditions. High rotational speeds like 17000 rpm and feed rates of up to 210 mm/min exacerbate stress on the outer corner when cutting moulds with hard inclusions present.
A point angle of 118 degrees concentrates force at the tip, making it more susceptible to chipping during interrupted cuts or sudden changes in material hardness. Reducing feed rate and adjusting cut entry angles can mitigate damage but a stronger edge preparation is essential for maintaining tool integrity.
The order to check things
Start by checking if chipping at the outer corner is due to material hard inclusions or interrupted cutting entry. Such conditions often cause initial wear on this part of the tool. If chipping persists, adjust the feed rate and cutting speed within recommended limits for DC836L. Lower speeds and feeds reduce stress concentration at the outer corner. Next, inspect the edge preparation on your tools.
A stronger edge preparation helps resist chipping better than a harder coating under harsh conditions. If a stronger edge is not sufficient, consider changing to a tool with a higher HRC hardness rating from DC836L’s range. Higher hardness can improve wear resistance but may increase brittleness. This order—checking material, adjusting speeds, evaluating edge prep, and finally choosing harder carbide—is based on cost-effectiveness and likelihood of success. Start simple before moving to more expensive solutions.
Confirming the cause before changing anything
Before changing parameters, inspect for hard inclusions or interruptions at entry causing initial chipping. Hard inclusions increase load on the tool edge, which leads to premature wear and damage. Check if interruptions occur when entering the material, adding sudden stress peaks to carbide. A stronger edge preparation can handle these conditions better than a harder coating alone. Review tool marks for signs of hard inclusion impact or abrupt entry stress before adjusting settings.
After confirming chipping is due to inclusions or interruptions, consider using DC836L with optimal geometry. Ensure the cutting speed and feed rate match material properties and machine capabilities accurately. Adjustments may include reducing cutting speed or increasing tool engagement for smoother entry. Testing at lower speeds or feeds can help determine if conditions causing chipping are mitigated. Monitor the outer corner carefully during tests to verify improvements in edge durability and performance.
Frequently asked
Why does chipping happen at the outer corner of my carbide cutting tools?
Chipping occurs at the outer corner due to high speeds and heavy loads, especially if there are hard inclusions or interruptions during entry. A stronger edge preparation is more effective than a harder coating for preventing this issue.
How can I prevent chipping on the outside edges when using DC836L carbide tools?
To avoid chipping, use a tool with enhanced edge durability rather than relying solely on hardness. For DC836L tools, ensure correct speeds and feeds within specified ranges to reduce stress on the outer corner.
What is the right point angle for my cutting tool to prevent chipping at high speeds?
A 118° point angle reduces forces during cutting, helping to minimise chipping even at high speeds. Stick to recommended rpm and vc values to maintain optimal performance and edge integrity.