51 articles in this category. Browse the full library for application, process and product notes across the catalogue.
In mould steel the coating has to resist abrasion at a temperature that is high but not extreme, which is the range where a bronze layer works well and a DLC...
Run the same speed with both coatings and the difference is temperature. AlTiN forms an oxide layer that keeps the coating from breaking down; TiCN oxidises...
TiN and TiCN differ less in hardness than in where that hardness survives. TiN keeps its hardness higher up the temperature scale; TiCN is harder at the temp...
Below 0.3 mm the coating thickness becomes a significant fraction of the edge radius, so coating a micro drill changes its geometry. That trade-off is why un...
A thicker coating wears longer and rounds the edge more. On a micro drill the second effect matters more than the first, because an edge radius that grows by...
Titanium reacts with most coating materials at cutting temperature, so the coating that protects a steel tool can dissolve on a titanium job. The useful ques...
Stainless is the material where coating choice is most often got wrong, because the dominant failure is adhesion rather than wear. A coating that resists abr...
Both are wear layers on the same carbide, and the difference appears in the wear pattern rather than in the initial performance. A bronze layer tends to thin...
Both avoid the adhesion problem that plagues nitride coatings in aluminium. The difference is durability: an uncoated edge can be ground sharper and repolish...
Titanium is chemically aggressive and DLC is chemically inert, which sounds like a match. In practice the low thermal stability of DLC limits it to low-speed...
CFRP is abrasive and its resin softens with heat. DLC keeps the edge sharp while reducing friction against the resin, which limits the heat that causes the r...
Copper adheres to almost any clean surface. A DLC layer presents a low-energy surface that copper does not wet as readily, which is the mechanism by which it...
DLC is chosen in aluminium for its low friction coefficient against the work, which reduces the welding that forms a built-up edge. It is not chosen for hard...
Hardened steel above HRC 40 wears the coating quickly whatever it is, so the choice comes down to which coating fails progressively rather than catastrophica...
A black coating is a wear layer that also reduces friction against the chip. It is a practical default for carbon steel where the exact coating composition m...
Bronze coatings perform well against the abrasive carbides in alloy steel. Their advantage over TiN grows as the alloy content rises and the wear mechanism s...
A bronze coating is chosen in stainless for its balance of wear resistance and low adhesion. It also leaves a wear pattern that is easy to read, because the...
Mould steel at HRC 30 to 40 is abrasive and hot. A black wear layer sits between TiN and TiCN in performance and is often chosen when the job mixes mould ste...
Stainless needs a coating that resists adhesion as much as wear. A black layer reduces the tendency for stainless to weld to the rake face, which delays the...
In PCB drilling the coating's job is to resist glass-fibre abrasion without changing the edge geometry. A black wear layer keeps the point intact through tho...
Hardened steel generates heat at the edge even at moderate speed. AlTiN tolerates that temperature better than TiCN, but the trade-off is a coating that is m...
At high cutting speed the edge reaches a temperature where TiN and TiCN oxidise. AlTiN keeps its hardness further up the temperature scale, which is the only...
Nickel alloys hold heat at the edge and attack the tool chemically. AlTiN's hot hardness and oxide layer are the closest thing to protection, but the notch t...
AlTiN forms an aluminium oxide layer at temperature that slows the chemical reaction between the tool and titanium. It buys time, not immunity: the speed sti...