A thicker coating extends tool life by reducing wear. However, on micro drills, it also increases edge radius significantly, affecting cutting efficiency and chip control critically. For DC426 drills with diameters from 0.04 to 3 mm, this means the coated edge can round off too much, hindering performance at high speeds and feeds. As a result, choosing an optimal coating thickness is crucial for maintaining sharp edges necessary for precise drilling operations in tight tolerances.
What the coating does in this cut
The black coating on DC426 drills enhances wear resistance, raising tool life at high speeds like 25000 rpm and feeds up to 75 mm/min. Coatings with hardness ranging from 89–93 HRC form a barrier against abrasive materials during drilling operations, protecting the carbide substrate. This layer does not change the drill's geometry; it remains at 135° point angle for all diameter sizes from 0.04 mm to 3 mm.
While wear resistance increases, thicker coatings add more material to the cutting edge, increasing its radius by micrometres on small drills like those in the DC426 series. This added edge radius reduces sharpness and affects chip formation and cutting efficiency at lower speeds around 15000 rpm and higher feeds of 750 mm/min.
| Specification | Value |
|---|---|
| Point angle | 135 ° |
| Carbide hardness | 89–93 HRC |
| Series diameter range | 0.04–3 mm |
The chemistry between coating and workpiece
At high temperatures, chemical reactions between the coating and workpiece alter wear patterns on DC426 drills. Iron-based carbides form at 750 mm/min feed rates when drilling carbon steel. These compounds reduce cutting edge sharpness more than expected, changing tool geometry over time. The point angle of 135 degrees remains constant but effective edge radius increases due to these reactions. Carbide substrate hardness between 89 and 93 HRC resists deformation under high pressure at speeds up to 100 m/min.
However, coating integrity degrades faster than the substrate when cutting forces rise sharply. As temperatures exceed 500 degrees Celsius during drilling operations, oxidation occurs on the black titanium carbonitride (TiCN) layer. This process thickens the initial 2-3 micrometre coating to around 4-6 micrometres after extended use. Thicker coatings provide better thermal insulation for the carbide substrate but also introduce more material into contact with the workpiece surface, which leads to increased wear from chemical interactions at cutting edges.
How it fails
The black coating on DC426 drills wears due to friction and high temperatures, reducing its thickness over time. This wear is more pronounced at higher speeds like 25000 rpm and feeds up to 75 mm/min. As the coating thins, it exposes the carbide substrate, which has a hardness of 89–93 HRC. The exposed substrate then begins to wear from cutting forces and heat generated during drilling operations. At lower speeds such as 15000 rpm, this process happens more slowly compared to higher speeds.
Chemical reactions between the coating and workpiece create iron-based carbides at high feeds like 750 mm/min, altering the usual wear pattern. These reactions can cause premature failure of both coating and substrate if not managed properly through appropriate cutting conditions. Micro drills with a 135-degree point angle are especially sensitive to these changes in edge radius. Substrate wear typically occurs after prolonged use or under extreme conditions, which leads to increased tool diameter and reduced accuracy. Effective maintenance and monitoring of drilling parameters can extend the useful life of coated micro drills by preventing excessive substrate exposure and wear.
Choosing between the available options
When choosing a coating thickness for DC426 drills, consider the tool life requirements at your operating conditions. Higher hardness coatings like those in the 90–93 HRC range offer better wear resistance than softer ones. At lower speeds up to 18000 rpm and feeds of 50 mm/min or less, thinner coatings suffice due to reduced frictional heat. Above these parameters, thicker coatings provide extended durability by resisting higher temperatures and chemical reactions with the workpiece material. For micro-drills, a thicker coating rounds the edge more noticeably over time, affecting cutting accuracy significantly.
Smaller diameter drills require careful selection to balance wear resistance against potential loss of sharpness. When operating at extreme speeds like 25000 rpm or feeds up to 75 mm/min, opt for the thickest available coating on DC426 to maintain edge integrity and prolong tool life. Higher temperatures accelerate wear patterns that can degrade performance rapidly without adequate protection. Consider testing a range of coatings under your specific conditions to determine optimal thickness before full-scale production starts. This approach helps in identifying the most suitable balance between durability and cutting precision for your application needs.
Frequently asked
How does coating thickness affect drill performance?
Thicker coatings wear out slower but cause more edge rounding, especially on micro drills where small changes matter significantly. This affects cutting precision and tool life.
What is the optimal point angle for carbide drills?
A 135-degree point angle balances stability and sharpness for most drilling tasks with carbide tools. It provides good centreing and wear resistance without sacrificing chip clearance.
Which RPM settings should I use for carbon steel?
For carbon steel, use higher speeds like \(25000 \text{ rpm}\) for smaller drills down to \(15000 \text{ rpm}\) as diameter increases. Adjust feed rates accordingly based on drill size and material hardness.