ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION
Technical library · 512 published articles

Engineering notes

Application notes, process notes and product notes from the TONNY engineering team. Each article ties a catalogue geometry to the operation it performs and the failures it prevents.

Articles512published
Categories10topics
Latest2026-11-20published
EditionENlanguage

04Notes, page 4 of 22

24 articles on this page
Failure analysis

Fibre pullout in CFRP

CFRP fails by fibre pullout when the edge is dull enough to push fibres aside rather than shear them. The hole looks furry rather than torn, and the fibres t...

4 min read ·
Cutting parameters

CFRP speed and resin temperature

The fibre tolerates almost any speed; the resin does not. Speed is set by the temperature at which the matrix softens, which is well below the temperature a...

4 min read ·
Cutting parameters

Graphite speed and dust management

Graphite allows high speed because it does not soften, but the dust it produces is abrasive and unhealthy. Extraction and enclosure matter more than the cutt...

4 min read ·
Material selection

Drilling 0.3 mm holes in nickel-based alloy

At 0.30 mm the tool is strong enough to survive an imperfect setup, so the process limits move from the tool to the machine and the fixture. Nickel alloys ha...

3 min read ·
Material selection

Drilling 0.2 mm holes in graphite

At 0.20 mm the flute just has room to carry a chip, which makes evacuation possible for the first time in the micro range. Graphite removes as an abrasive du...

5 min read ·
Cutting parameters

Speed limits set by melting, not by wear

Plastics do not wear a carbide edge, they melt onto it. Speed has to stay below the point where friction heat exceeds what the chip can carry away, which is...

4 min read ·
Material selection

Drilling 0.3 mm holes in PCB laminate

At 0.30 mm the tool is strong enough to survive an imperfect setup, so the process limits move from the tool to the machine and the fixture. PCB laminate is...

4 min read ·
Coatings

DLC coating for titanium alloys

Titanium is chemically aggressive and DLC is chemically inert, which sounds like a match. In practice the low thermal stability of DLC limits it to low-speed...

3 min read ·
Failure analysis

Resin smear in PCB holes

Resin smeared across the copper Barrel is a heat problem: the resin softens and is wiped along the wall by the margin. Lower speed and a sharper edge reduce...

5 min read ·
Failure analysis

Glass fibre abrasion in PCB

Glass fibre is harder than the cobalt binder, so it wears the tool by abrasion at a rate that rises steeply with speed. Tool life in PCB drilling is counted...

3 min read ·
Cutting parameters

Stainless speed and the work-hardening trap

Too slow in stainless means rubbing, and rubbing hardens the surface the next pass has to cut. There is a window where the tool cuts under the hardened layer...

4 min read ·
Material selection

Drilling 0.3 mm holes in copper alloy

At 0.30 mm the tool is strong enough to survive an imperfect setup, so the process limits move from the tool to the machine and the fixture. Copper conducts...

4 min read ·
Failure analysis

How 0.4 to 0.6 mm drills fail

When a tool in this band fails early it is usually because the point geometry does not match the material — a 118-degree point in a hard alloy raises thrust...

3 min read ·
Failure analysis

How 10 to 14 mm drills fail

The failure mode is margin wear plus heat, and the symptom is a hole that grows oversize progressively. A tool that is dull at this size makes a lot of heat...

3 min read ·
Failure analysis

Delamination in PCB laminate

A PCB stack is glass fibre, resin and copper bonded together, and the bond fails before the fibres cut if the point angle is too blunt. Delamination starts a...

4 min read ·
Material selection

Drilling 0.3 mm holes in pre-hardened mould steel

At 0.30 mm the tool is strong enough to survive an imperfect setup, so the process limits move from the tool to the machine and the fixture. Mould steel at H...

4 min read ·
Coatings

DLC coating for carbon-fibre composite

CFRP is abrasive and its resin softens with heat. DLC keeps the edge sharp while reducing friction against the resin, which limits the heat that causes the r...

4 min read ·
Cutting parameters

Keeping titanium speed low on purpose

Titanium's low conductivity means the heat stays at the edge, so speed is limited by the tool's tolerance for temperature rather than by the workpiece. Runni...

4 min read ·
Failure analysis

Edge spalling in ceramics

The edge spalls because the ceramic is harder than the tool and the load is intermittent. Once a piece of the edge leaves, the tool rubs and the hole becomes...

3 min read ·
Coatings

DLC coating for copper alloys

Copper adheres to almost any clean surface. A DLC layer presents a low-energy surface that copper does not wet as readily, which is the mechanism by which it...

5 min read ·
Material selection

Drilling 0.2 mm holes in hardened steel at HRC 45

At 0.20 mm the flute just has room to carry a chip, which makes evacuation possible for the first time in the micro range. The tool no longer cuts much harde...

4 min read ·
Material selection

Drilling 0.3 mm holes in alloy steel

At 0.30 mm the tool is strong enough to survive an imperfect setup, so the process limits move from the tool to the machine and the fixture. Alloy steel carr...

4 min read ·
Failure analysis

Wear that is not wear

Discolouration, coolant residue and coating transfer can all look like a wear land under a loupe. Cleaning and re-examining before changing a parameter saves...

4 min read ·
Failure analysis

How 4 to 6 mm drills fail

Corner and margin wear set life. At this diameter a worn margin rubs the hole wall and generates heat, so the tool fails from the outside in, and regrinding...

4 min read ·
About this library

Articles are written against the production catalogue. Dimensions and part numbers referenced in the text resolve to the same records used by the series and diameter pages.