Discoloured workpieces around holes indicate heat transferred into the part rather than removed with chips, typically due to insufficient feed rate or excessive cutting depth. High hardness of DC426 tools—between 89 and 93 HRC—ensures durability despite challenging conditions. A point angle of 118 degrees optimizes chip evacuation for these small diameters. Proper feeding rates from 30 mm/min to 150 mm/min help manage heat effectively, preventing discoloration by distributing it through the chips. Using recommended spindle speeds ensures optimal chip thickness and minimizes friction that could otherwise cause overheating.
The symptom as it appears
A blue or brown discoloration appears around the hole on the workpiece after drilling. This discolouration indicates that excessive heat transferred into the part rather than being carried away with the chips. Light feed rates cause more friction between the cutting edge and the material, generating higher temperatures at the point of contact. Insufficient coolant flow also exacerbates this issue by failing to dissipate heat effectively from the workpiece surface. Dark marks are often visible on the drill's cutting edges where they contacted the hot workpiece area. These marks can indicate wear or slight damage to the edge geometry and coating.
Checking for signs of wear is crucial before proceeding with further operations. The DC426 series, designed with a black coating, provides excellent heat resistance during machining processes involving stainless steel. However, even these tools show discoloration under inadequate feed rates or coolant conditions. Inspecting the workpiece reveals that discoloured areas are typically located near the exit point of the hole, where most of the friction occurs between the drill and material surfaces. This location highlights the critical need for proper cutting parameters to minimize heat generation.
| Specification | Value |
|---|---|
| Point angle | 118 ° |
| Carbide hardness | 89–93 HRC |
| Series diameter range | 0.04–3 mm |
What can produce that symptom
A blue or brown discoloration around a hole indicates excessive heat transferred into the workpiece instead of being removed as chips. Insufficient feed rate is often the cause, leaving more heat in the part than expected. High hardness and sharp geometry help reduce cutting temperatures but cannot compensate for inadequate chip clearance. A tool with an 118-degree point angle efficiently removes material but requires proper feed rates to manage heat effectively. Using a higher feed rate as per the recommended data reduces discoloration by removing more heat through increased chip volume.
Increasing feed rates, especially when drilling stainless steel, ensures that heat is removed from the workpiece rather than remaining in it. Feed settings of 30 mm/min for high speeds and up to 150 mm/min at lower speeds minimize discolouration issues. Matching your spindle rpm to our recommended range also prevents excessive heat transfer into the material. Proper cooling or lubrication can further assist in managing elevated temperatures during cutting operations. Regularly inspecting tools helps maintain optimal geometry, ensuring consistent performance and reducing discoloration symptoms.
The order to check things
Check feed rate first because insufficient feed causes heat to remain in the workpiece. Feed rates of 45 mm/min or higher should prevent discolouration for most materials. Reduce speed if increasing feed does not help, starting with the highest recommended rpm settings. A lower cutting speed can also reduce heat transfer into the part. Check geometry next; a point angle of 118 degrees balances strength and chip evacuation effectively.
Ensure correct tool diameter matches your hole size requirements precisely. Verify that cutting fluid application is adequate as insufficient cooling exacerbates discolouration issues. Use recommended amounts to manage temperature during drilling operations properly. Finally, inspect the workpiece material properties for any deviations from standard specifications. Unexpected hardness or alloy composition changes may require adjustments in feed and speed settings.
Confirming the cause before changing anything
To confirm a heat issue before changing parameters, measure the feed rate first. Use a digital caliper to measure chip thickness accurately at the cutting edge.
A thicker chip means less heat stays in the workpiece. Compare actual chip thickness with calculated values from your drilling data.
Frequently asked
Why is there discolouration around the hole after drilling?
Discolouration indicates excessive heat transferred to the workpiece rather than the chip, often due to too light feed rates. Adjusting the feed rate can help manage this issue.
What hardness should my carbide drill have for stainless steel?
For drilling stainless steel, a carbide hardness of 89-93 HRC is optimal, providing both durability and edge retention needed for hard materials.
How do I set up cutting parameters to avoid discolouration?
Use feed rates between 30 to 150 mm/min with spindle speeds from 7000 to 15000 rpm. Adjust the speed based on material thickness, using values like vc = 60-120 m/min and fz as per tool specifications.