Using a DC826 tool with an 118-degree point angle reduces thrust and minimizes cracks from excessive pressure during brittle material cutting. Hardness between 1800–2000 HV ensures durability while maintaining flexibility against thermal shock in carbon materials.
The symptom as it appears
Cracks appear as fine radial lines originating from a drilled hole in the workpiece, extending towards the edges. These cracks are most visible after drilling through thin brittle materials like carbon steel at high speeds. Using too much thrust during cutting can cause microfractures that propagate along grain boundaries. A slower feed rate and lower rotational speed help reduce thermal shock, minimizing crack formation. Radial cracks also indicate an overheated tool edge, often seen near the point angle of 118 degrees.
Applying proper coolant or increasing dwell time between cuts cools the cutting zone effectively. The uncoated DC826 tools show wear marks and minor chipping around the entry point after extended use at high feed rates. These signs indicate that optimal cutting parameters have not been maintained consistently. Maintaining cutting data within recommended limits prevents excessive tool wear and reduces risk of crack formation in workpieces. For instance, starting with a lower feed rate can help stabilize initial cut conditions.
| Specification | Value |
|---|---|
| Point angle | 118 ° |
| Carbide hardness | 1800–2000 HV |
| Series diameter range | 0.13–10.3 mm |
What can produce that symptom
Cracks radiating from a hole indicate excessive cutting thrust or thermal shock during machining of brittle materials like carbon. This occurs when the tool's entry into the material generates high localized stress. Using an 118-degree point angle spreads this force over a larger area, reducing pressure concentration. A slower feed rate minimizes sudden temperature changes that can cause thermal shock. For optimal results, decrease spindle speed to reduce cutting forces and heat generation.
When machining at higher speeds like 25000 rpm, the risk of thermal damage increases due to rapid heating and cooling cycles. Switching to lower speeds such as 18000 rpm or 15000 rpm can help mitigate these effects. Feeding material into the cut slowly, for example at 75 mm/min instead of 50 mm/min, allows more time for heat dissipation. Maintaining a cutting speed below 180 m/min further protects against thermal stress. Adjusting parameters in this manner prevents radial cracks from forming around drilled holes.
The order to check things
Begin by checking if feed rates are too high for your material hardness. Lowering feed rates reduces thrust and can prevent cracks in brittle materials. Next, verify whether the rpm settings match the tool's capabilities. Running at 15000 rpm rather than higher speeds helps manage heat buildup and minimizes thermal shock. Adjust the point angle if initial checks fail to resolve cracking issues.
A steeper point angle spreads cutting forces more evenly across the workpiece surface. Review your coolant application technique next. Proper cooling reduces temperature spikes, preventing thermal stress that can cause radial cracks around holes. Finally, consider tool wear as a potential source of increased thrust and heat generation. Regularly replacing worn tools maintains optimal cutting conditions and minimizes cracking risks.
Confirming the cause before changing anything
Before adjusting any parameters, perform a trial cut with standard settings. Use a DC826 tool at 180 m/min cutting speed for carbon material.
Reduce feed rate gradually until cracks no longer appear on the workpiece surface. Measure thrust force using a dynamometer to confirm excessive load.
Frequently asked
How do I prevent cracks from forming around holes when drilling?
Use a steeper point angle and slower feed rates to distribute thrust more evenly and reduce thermal shock. For brittle materials, choose a drill like DC826 with an 118° point angle.
What causes cracks during the drilling process?
Cracks usually form due to excessive cutting forces or rapid temperature changes causing thermal shock in hard, brittle materials. Adjusting feed rates and spindle speeds helps mitigate these issues.
Can you recommend optimal settings for carbide drills to avoid cracks?
Set your drill at 180 m/min speed and use a slower feed rate of 75 mm/min when working with brittle materials like carbon steel. Opt for DC826 series with an HV range of 1800-2000 for better performance.