ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

A drill that breaks at the point

A point failure is a thrust problem: too much feed, a dull edge, or a web that is too thick for the material. The break face tells you whether it failed in t...

4 min read 746 words Updated 2026-08-15
A snapped micro drill on a bench beside its broken tip — A drill that breaks at the point

A drill with an 118-degree point angle and hardness from 89 to 93 HRC prevents thrust failures by maintaining cutting edge integrity under high feed rates and speeds. This robust geometry minimizes web thickness, reducing compression failure risk when drilling through hard materials. With optimal spindle speeds of 20000 rpm down to 9000 rpm for alloy steels, the drill ensures consistent chip formation and wear resistance. Feed rates from 40 mm/min up to 270 mm/min accommodate various material densities without compromising tool longevity or surface finish quality. The bronze coating on DC836 series enhances lubricity and thermal stability, further protecting against point breakage during operations.

The symptom as it appears

A dull or damaged cutting edge on a DC836 drill causes excessive force during drilling, which leads to breakage at the point. Point failure appears as visible cracks and chips on the tip of the tool. These defects initiate from high feed rates and inadequate coolant application. The fractured area shows signs of compression stress near the web. This indicates that the material could not withstand the applied pressure.

On the workpiece, a broken DC836 drill leaves rough, uneven holes with burrs around the edges. The hole diameter may also be slightly larger than intended. Inspecting the drill reveals a thin and weakened cutting edge after point failure occurs. Proper maintenance and adherence to recommended cutting parameters prevent such issues.

SpecificationValue
Point angle118 °
Carbide hardness89–93 HRC
Series diameter range0.1–14 mm

What can produce that symptom

A drill with a thick web relative to its diameter can cause point failure due to excessive compression forces during cutting.

The DC836's geometry is optimized for specific material hardness ranges; deviations from these ranges increase the risk of breaking at the point.

The order to check things

Start by examining feed rate and spindle speed settings for accuracy relative to cutting data guidelines. Verify that no excessive forces are applied, potentially causing edge damage. Inspect the drill's cutting edges for signs of wear or chipping before use. If the web thickness is too large compared to diameter, adjust drilling parameters accordingly. Consider reducing the feed rate if point failure occurs despite correct settings and condition.

If initial checks do not identify issues, test with a new DC836 tool in similar conditions. Observe break patterns for clues about the cause of failure. A compressed fracture suggests excessive material hardness or improper feed rate. Conversely, a twisted break indicates over-torquing at high speeds. Adjust drilling parameters based on observed damage and consult cutting data for optimal performance.

Confirming the cause before changing anything

The DC836's geometry is designed with a 118-degree point angle for optimal performance in various materials. Ensure that the feed rate does not exceed recommended values to prevent excessive compressive forces at the cutting edge. Verify spindle speeds are within specified limits to avoid overloading the drill bit during operation. Inspect the cutting edge for signs of wear or damage, as these can lead to increased thrust and breakage. Check the drill's web thickness relative to diameter; a thicker web can cause compression failure under high forces.

Use a microscope to examine the fracture surface on the broken point. A shear lip indicates torsional failure from excessive torque, while cracks spreading radially suggest compressive overload. Adjust parameters accordingly once the specific type of failure is identified. For torsional failures, reduce feed rates or increase spindle speeds as needed. In cases of compressive overload, consider using a drill with a thinner web or adjust material hardness and machinability ratings for better compatibility.

Frequently asked

Why does my carbide drill break at the point?

Point failure typically indicates issues like excessive feed, dull edges, or an overly thick web for the material being drilled. Check if the break face shows torsion or compression failure and adjust your cutting parameters accordingly.

What are the correct rpm settings for a DC836 drill?

For optimal performance with the DC836 series, use 20000 rpm for soft materials, 13000 rpm for medium-hardness alloys, and 9000 rpm for harder metals. Adjust based on material type and cutting conditions.

How do I prevent my carbide drill from breaking?

Prevent breakage by ensuring the correct point angle of 118° and maintaining proper feed rates within recommended ranges. Use lower speeds and higher feeds for tougher materials to avoid excessive stress on the tool.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index