ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Coating worn through in a band

A wear band at a fixed distance from the point usually means the tool is rubbing at that depth, not that the coating is poor. The band marks the depth where...

4 min read 832 words Updated 2026-08-27
Close-up of a worn carbide drill edge with a visible wear land — Coating worn through in a band

A wear band on a carbide tool indicates rubbing rather than poor coating quality. This occurs where chip clearance stops, typically at depths of cut around 0.04 mm to 3 mm for DC426L tools. At these settings, the band shows where the tool's rake angle and cutting speed compromise chip flow. Understanding this helps operators adjust feed rates or speeds to prevent overheating and maintain tool life. Recognizing rubbing patterns enables better process control and reduces waste from premature tool replacement.

The symptom as it appears

A wear band appears on the tool’s cutting edge after prolonged use at specific depths of cut. This marks where continuous rubbing occurs rather than normal cutting action. The band usually starts near the tip and progresses toward the shank as usage continues. Depth of cut too shallow or feed rate insufficient causes this condition, not coating failure. Surface finish deteriorates in areas corresponding to the wear band location on the tool.

Machined surfaces show irregularities matching the tool’s worn profile at those depths. For stainless steel machining, common band formation occurs around 0.1 mm depth of cut when rpm and feed parameters are set improperly. Adjusting these settings can prevent or delay band appearance. Worn-through coating reveals underlying carbide substrate, accelerating wear and reducing tool life significantly. This exposes the softer material to abrasive forces, causing rapid deterioration.

SpecificationValue
Point angle118 °
Carbide hardness89–93 HRC
Series diameter range0.04–3 mm

What can produce that symptom

A wear band forming at a constant depth suggests continuous rubbing, often due to inadequate chip clearance at that level. This is common when cutting depths exceed the optimal range for proper chip formation and evacuation. Excessive feed rates or insufficient spindle speeds can exacerbate this issue by failing to maintain adequate chip thickness control. For stainless steel, feeds between 30 mm/min and 55 mm/min are generally suitable for maintaining good chip clearance at recommended depths of cut. Higher speeds above 120 m/min may also contribute if not balanced with appropriate feed rates to prevent overheating and poor lubrication.

Lower spindle speeds below 7000 rpm might cause thicker chips, which leads to inefficient cutting and increased friction against the workpiece surface. Tools like DC426L have a geometry designed for efficient chip removal but require adherence to specified cutting parameters for optimal performance. Adjusting feed rates to match the tool’s capabilities ensures continuous, smooth chip flow, reducing the risk of wear bands forming prematurely. Proper adjustment of these variables helps maintain tool longevity and machining efficiency by preventing localized overheating and mechanical stress buildup.

The order to check things

Check the chip clearance groove first when a wear band appears at a constant depth. This groove should ensure chips do not build up at that location. Ensure adequate coolant flow next; insufficient cooling can cause accelerated tool wear in this area. Adjust feed rate or cutting speed if needed to improve conditions here. Inspect for correct workpiece alignment and setup next, as misalignment might force the tool into rubbing at specific depths.

A properly aligned machine reduces unnecessary stress on the tool edge. Compare actual cutting parameters with recommended values from the data sheet. Deviations could lead to excessive heat generation and premature wear in the same spot repeatedly. Lastly, consider replacing worn or damaged components like holders before suspecting issues with the coating itself. This approach saves costs by addressing simpler causes first.

Confirming the cause before changing anything

Inspect the chip clearance groove carefully before altering any cutting parameters. Ensure chips flow freely without building up at the wear band location. If chips are obstructed, increase the depth of cut slightly or adjust the feed rate accordingly. This change should improve chip evacuation and reduce rubbing. Check tool geometry to ensure it matches recommended specifications for optimal performance.

Confirm point angle is 118 degrees as deviations can cause poor chip control. Run tests with unchanged parameters after addressing clearance issues. Observe if wear band persists at same location or moves, indicating the root cause of the problem. Document all findings and adjustments made during testing phases. This record helps in future troubleshooting by providing a clear history of changes and outcomes.

Frequently asked

What does it mean when the coating wears through in one band?

A worn-through coating at a fixed depth usually indicates rubbing rather than poor coating quality. This marks where chip clearance stops, not coating failure. Adjust cutting parameters for better performance.

Why does my carbide tool show wear only on one side?

Uneven wear often results from improper setup or inconsistent material hardness. Ensure correct feeds, speeds, and coolant application to minimize this issue.

How do I prevent premature wear bands on my cutting tools?

To avoid premature wear bands, use optimal cutting parameters for your specific materials. Adjust feed rates and spindle speeds according to tool specifications to maintain performance.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index