ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Failure analysis: Delamination at hole entry and exit

Delamination is a layered material separating under the thrust of the point. It is worst at entry before the tool is fully engaged and at exit when the suppo...

3 min read 628 words Updated 2026-02-16
Cross-section of a drilled metal block showing the hole wall — Failure analysis: Delamination at hole entry and exit

Delamination reduces hole quality by causing layers to separate under cutting forces, most severely at entry and exit points where material support is weakest. Increasing the point angle from 150 degrees to 160 degrees enhances stability and minimizes layer separation because it spreads these critical forces over a larger area. This geometry change does not significantly affect chip clearance or tool diameter; the HDC636 maintains its 0.3 mm size while improving resistance to delamination stress. By mitigating initial and final entry pressures, this design prolongs tool life and ensures consistent hole dimensions across various materials and depths.

The symptom as it appears

On parts with delamination, layers split at entry and exit points, visible as a rough surface around holes.

Delaminated surfaces show distinct raised edges where material has separated from underlying layers.

SpecificationValue
Point angle150 °
Point angle160 °
Diameter0.3 mm
Carbide hardness1800–2000 HV

What can produce that symptom

Delaminated surfaces show distinct raised layers at hole entry and exit points due to insufficient material support during cutting.

Excessive pressure from a steep point angle, like 150 degrees, exacerbates delamination by concentrating forces narrowly on the entry surface.

The order to check things

To address delamination effectively, start with the least costly option: adjusting peck drilling parameters first. This reduces peak cutting forces at entry and exit points. Next, consider using a point angle of 160 degrees instead of 150 degrees for better stress distribution. A wider angle spreads out forces more evenly across the material surface. If delamination persists despite these changes, introduce a carbide backing plate to support workpiece edges during cutting.

This external support stabilizes the area around entry and exit points. Check the hardness range of your carbide tool; ensure it falls within 1800–2000 HV for optimal durability without brittleness issues. Proper hardness balances wear resistance with fracture toughness. Finally, inspect parts thoroughly before production runs to avoid using damaged or substandard materials that may exacerbate delamination problems at critical points.

Confirming the cause before changing anything

To confirm delamination caused by insufficient support at entry and exit points, test with a backing plate before altering any drilling parameters. A backing plate provides continuous support beneath the workpiece, reducing stress on thin or unsupported material edges. It also helps maintain consistent feed rates during peck cycles. For tools without a backing plate, try increasing the point angle to 160 degrees. A wider angle distributes cutting forces over a larger area, decreasing local stress concentrations at entry and exit points.

This adjustment alone often reduces delamination significantly. If delamination persists, consider using HDC636 with its steeper 150-degree point angle for harder materials that require aggressive cutting. Ensure the tool diameter matches the hole size precisely. A 0.3 mm diameter drill should produce holes of exactly 0.3 mm to minimize unsupported material layers around entry and exit points.

Frequently asked

Why does delamination happen at hole entry and exit?

Delamination occurs when thin layers of material separate due to stress from cutting tools, especially at entry and exit points where support is weakest. A steeper point angle like \(160^\circ\) helps reduce this issue compared to a shallower one like \(150^\circ\).

What causes delamination during drilling?

Delamination happens when layers in the material separate due to excessive stress, typically at hole entry and exit where support is limited. Using shorter peck cycles or applying a backing plate can mitigate this problem.

How do different point angles affect delamination?

A \(160^\circ\) point angle reduces delamination risk compared to a \(150^\circ\) angle by providing better support as the tool enters and exits the material, reducing stress on thin layers.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index