ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Exit delamination in CFRP

At exit the unsupported fibres bend away from the tool and delaminate before they are cut. A backing plate or a reduced feed at breakthrough addresses it; in...

3 min read 675 words Updated 2026-10-10
Carbon fibre composite panel edge with a drilled hole — Exit delamination in CFRP

Carbide tools with a 130-degree point angle reduce exit delamination by minimizing unsupported fibre bending at CFRP breakthrough. This geometry supports controlled material flow, preventing fibres from splitting away from the tool. Lowering feed rates further enhances this effect, as slower feeds allow more time for fibres to align properly before cutting. Tools like DC336 maintain consistent performance across various diameters and coating types. High hardness in carbide—1800 to 2000 HV—enables precise cuts without compromising durability.

The mechanism

Carbide tools with a 130-degree point angle enter the material at an acute angle, minimizing unsupported fibre length. This geometry reduces bending stresses on fibres during cutting entry and exit. Fibre delamination occurs when bent fibres separate before being cut by the tool edge. A backing plate supports fibres near breakthrough, preventing premature separation. Decreasing feed rate at exit also reduces bending forces on remaining fibres.

Carbide hardness in the range of 1800 to 2000 HV ensures durability against wear and tear during cutting. Lowering rotational speed from 25000 rpm to 18000 or 15000 rpm reduces stress concentration at the exit point. A lower feed rate, such as 50 mm/min instead of 750 mm/min, further minimizes fibre bending forces. This combination helps maintain material integrity and prevents delamination during processing. Adjusting cutting parameters ensures optimal tool performance for various CFRP applications.

SpecificationValue
Point angle130 °
Carbide hardness1800–2000 HV
Series diameter range0.07–4.98 mm

The conditions that produce it

Carbide tools with a hardness range of 1800–2000 HV and a 130-degree point angle enter CFRP at an acute angle, minimizing unsupported fibre length. This geometry reduces bending stress on fibres as they exit the cut, thereby decreasing delamination risk. Operating at higher speeds like 180 m/min or lower feed rates such as 50 mm/min enhances this effect. Using a backing plate supports the material during breakthrough, further reducing exit delamination.

Increasing feed rate beyond 750 mm/min exacerbates fibre bending and can lead to more severe delamination issues. Reducing feed just before breaking through CFRP helps maintain support for fibres until they are fully cut, minimizing damage. Adjusting cutting parameters according to these guidelines ensures better material integrity at the exit point.

How to recognise it on the tool

Exit delamination appears on carbide tools as slight wear marks near the cutting edge at the exit point. These marks are faint but consistent with the material's hardness range of 1800–2000 HV. On parts, exit delamination causes surface cracks parallel to the cut direction where fibres pull away from the matrix. This often confuses users as tool wear or incorrect feed settings.

Using a backing plate helps reduce fibre bending at the end of cutting, mitigating these issues. Exit delamination can resemble edge chipping if not closely inspected. Both involve material loss near the exit point but differ in cause and appearance under magnification. Proper adjustment of feed rates just before breakthrough prevents further delamination without altering tool geometry.

What actually removes the cause

Reducing feed rate at exit can prevent delamination but decreases productivity and tool life significantly. Higher feed rates increase material removal, speeding up production times.

A backing plate supports fibres temporarily but cannot change entry geometry or fibre length effects. Using a DC336 tool with 1800–2000 HV hardness reduces unsupported fibre bending at entry.

Frequently asked

How do I prevent exit delamination when cutting CFRP?

Use a backing plate at the end of cuts or reduce feed rate as the material exits the cutter. Increasing feed worsens delamination because unsupported fibres bend and separate before being cut.

What hardness should my carbide tool have for CFRP?

Carbide tools for CFRP should be between 1800 to 2000 HV. This range balances wear resistance with toughness needed for composite materials.

Which geometry works right for cutting CFRP?

A point angle of 130 degrees is effective for CFRP due to its ability to reduce chip formation and heat generation, helping maintain material integrity during machining.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index