Drilling 0.8 mm holes in pre-hardened mould steel

At 0.80 mm the drill behaves like a drill: chips form and clear, and the tool can push a thin part out of position if it is not supported. Mould steel at HRC...

4 min read 839 words Updated 2026-11-01
A micro drill entering a clamped metal block on a machine table — Drilling 0.8 mm holes in pre-hardened mould steel

DC836L drills effectively at diameters from 0.14 mm to 14.2 mm, especially for HRC 30–40 mould steel. It maintains high hardness of 89–93 HRC, resisting wear on the flanks and heat in the substrate. The drill geometry optimizes chip formation at speeds up to 60 m/min and feeds from 35 to 210 mm/min. At 0.8 mm diameter, it handles chips efficiently while preventing part displacement during drilling operations. This ensures stable cutting performance and longer tool life compared to less durable alternatives.

The physics at this diameter

At 0.8 mm, the drill cuts through pre-hardened mould steel with HRC of 30 to 40 efficiently. The carbide edge retains hardness from 89 to 93 HRC under cutting forces. As it drills, chips form and clear out, preventing heat buildup on the tool flank. Increased rotational speeds up to 17000 rpm allow for faster material removal rates. Flank wear occurs due to abrasive particles in mould steel, shortening tool life.

At this diameter range, drilling dynamics change from smaller sizes significantly. Smaller drills rely more on chip breaking and coolant flow. Larger drills like 0.8 mm focus on maintaining structural integrity under higher torque demands. Cutting data shows feed rates vary from 35 to 210 mm/min for optimal performance. Speeds of 60 to 110 m/min optimize cutting efficiency while managing wear effectively.

SpecificationValue
Diameter0.6 mm
Diameter0.8 mm
Carbide hardness89–93 HRC
Series diameter range0.14–14.2 mm

What this material demands

At 0.8 mm diameter, DC836L drills pre-hardened mould steel with HRC 30 to 40 effectively. Hardness range of 89 to 93 HRC maintains edge sharpness during drilling operations. High drill speeds from 17000 rpm down to 7000 rpm ensure efficient chip formation. Chip clearance depends on feed rates: lower for slower speeds, higher for faster ones. Abrasive nature of pre-hardened steel causes wear mainly on the drill's flank and web.

DC836L carbide drill resists heat build-up due to its high hardness range of 89–93 HRC. Substrate softening occurs behind the cutting edge under prolonged use at high temperatures. Coolant application helps manage temperature rise, preventing substrate from degrading further. Flank wear limits tool life but does not affect hole quality until very late stages. Supporting thin parts during drilling prevents them from shifting and damaging the workpiece.

Tooling that fits the combination

DC836L uses a TiAlN coating that resists abrasive wear in hard steel. This coating enables higher cutting speeds compared to uncoated tools at similar hardness levels. The drill's geometry with an 0.8 mm diameter aligns chip thickness for optimal heat dissipation. Smaller diameters like 0.6 mm require finer adjustments for the same material. For pre-hardened mould steels, a TiCN coating might seem suitable but wears faster under high temperatures.

DC836L’s TiAlN coating remains effective even when substrate softens due to friction. Lower speeds and feeds can extend tool life in hard materials but reduce productivity significantly. Opting for higher rpm within the recommended range maximizes both durability and efficiency simultaneously. A positive rake angle helps control chip formation, preventing chips from re-cutting on the flanks. This feature is crucial at 0.8 mm diameter to maintain cutting accuracy throughout the process.

Cutting data and where it stops working

When drilling pre-hardened mould steel, cutting speed decreases first as hole size increases from 0.6 mm to 0.8 mm. At 0.8 mm, optimal rpm range narrows from 17000 to 7000 for stable cutting performance. Feed rate adjusts based on remaining hardness and tool stability requirements. Higher feed rates up to 210 mm/min are possible at lower speeds below 7000 rpm. Cutting speed must remain within 60 to 110 m/min range for effective chip formation and heat dissipation.

Tool wear initiates when the substrate softens due to high temperatures, affecting drill durability past optimal parameters. Abrasive particles in mould steel accelerate flank wear on carbide edge. Reduced hardness behind cutting edge compromises structural integrity of DC836L at extreme settings. Drilling stops working effectively if speed and feed rates exceed specified limits simultaneously. Proper setup within guidelines ensures right results for hole quality and tool life.

Frequently asked

How do I drill small holes in hardened steel?

For drilling 0.8 mm holes in mould steel at HRC 30-40, use DC836L carbide drills within their diameter range of 0.14 to 14.2 mm. Optimal settings are rpm = 7000 to 17000, vc = 60 to 110 m/min, and feed rate adjusted according to material hardness.

What is the right drill for HRC 30-40 steel?

DC836L carbide drills work well in pre-hardened mould steels. Use a feed of 50 mm/min or less depending on steel hardness. Ensure proper chip evacuation to prevent overheating and wear.

How do I avoid tool wear drilling small holes?

To minimise tool wear when drilling 0.8 mm holes, maintain optimal cutting parameters such as vc = 60-110 m/min and rpm settings appropriate for HRC 30-40 steel. Regularly inspect the drill's condition to prevent premature failure.

Data behind the text