ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Drilling 0.8 mm holes in titanium alloy

At 0.80 mm the drill behaves like a drill: chips form and clear, and the tool can push a thin part out of position if it is not supported. Titanium combines...

4 min read 817 words Updated 2026-10-30
Brushed stainless steel block with drilled holes — Drilling 0.8 mm holes in titanium alloy

DC426L drills 0.8 mm holes in titanium alloy with stability, thanks to its hardness range from 89 to 93 HRC. This ensures durability and wear resistance under high-temperature conditions. The drill's geometry matches the material removal rates suitable for titanium, maintaining cutting edge integrity. RPM options of 3000, 6000, and 10000 accommodate various workpiece thicknesses without sacrificing performance. With feed rates up to 80 mm/min, DC426L efficiently handles challenging drilling tasks in aerospace components.

The physics at this diameter

At 0.8 mm diameter, titanium alloy drilling requires careful control due to high thermal conductivity issues and chemical reactivity with coatings. Titanium's low thermal conductivity causes rapid edge wear as temperatures rise quickly near the cutting zone. Increased rotational speed within 3000 to 10000 rpm range reduces chip formation time but raises temperature risk. Black coating on DC426L helps resist titanium's reactive nature, enhancing tool longevity and performance stability.

As diameter increases from 0.6 mm to 0.8 mm, optimal feed rate shifts between 20 and 80 millimeters per minute for balanced cutting efficiency. Drilling thinner sections demands precise support to prevent part distortion or breakage during operation. Proper coolant application is crucial at these small scales to manage heat effectively and maintain edge sharpness. Geometry adjustments allow the tool to handle increased torque while maintaining structural integrity throughout the drilling process.

SpecificationValue
Diameter0.6 mm
Diameter0.8 mm
Carbide hardness89–93 HRC
Series diameter range0.04–3 mm

What this material demands

The drill's edge temperature rises quickly in titanium due to low thermal conductivity. Chemical reactions between titanium and coatings can weaken them rapidly at high temperatures. At 0.8 mm diameter, chips must clear efficiently to prevent clogging and reduce friction heating. Maintaining stability requires careful control of the cutting parameters within specified ranges. Hardness from 89 to 93 HRC helps resist wear but does not address chip formation issues directly.

Proper geometry ensures optimal chip evacuation and minimizes mechanical stress on the drill's tip. Coolant application becomes crucial as it reduces heat buildup and prolongs tool life in titanium drilling. Without adequate cooling, thermal expansion can affect dimensional stability and performance. Proper feed rates and spindle speeds must be balanced to manage cutting forces effectively. Too high a speed or too low a feed rate can lead to poor surface finish and increased wear.

Tooling that fits the combination

DC426L uses a geometry optimized for titanium drilling, with an 0.8 mm diameter ensuring efficient chip formation at high speeds up to 10000 rpm. At these rotations, titanium alloy’s low thermal conductivity causes rapid edge temperature increase, which leads to chemical reactions that degrade coatings more quickly than in steel. DC426L features a TiAlN coating resistant to titanium's aggressive chemistry and heat, maintaining cutting efficiency throughout the operation without premature wear issues.

A smaller 0.6 mm drill would be less stable at high speeds due to its reduced mass, risking vibration and poor hole quality when drilling through titanium plates. The larger diameter allows for optimal chip evacuation and reduces thrust forces, helping maintain part alignment even with thinner workpieces during cutting operations.

Cutting data and where it stops working

At 3000 rpm with a feed rate of 20 mm/min, drilling stability is maintained in titanium alloy due to lower temperatures and reduced chemical reactions at the cutting edge. Increasing the speed to 6000 rpm and doubling the feed rate to 40 mm/min intensifies heat generation but maintains chip clearance efficiency. This balance prevents rapid wear on the carbide tool. Further raising the drilling speed to 10000 rpm with a feed of 80 mm/min approaches the thermal limit; higher speeds lead to excessive edge temperatures and compromised coating integrity.

The process limit is reached when cutting values exceed these parameters, causing accelerated tool wear and potential failure. Proper coolant application mitigates temperature rise but does not extend the tool's life indefinitely. Each step-up in drilling parameters increases cutting efficiency initially but also elevates stress on the carbide material, reducing overall lifespan despite optimized geometry for titanium alloy.

Frequently asked

What is the right rpm for drilling 0.8 mm holes in titanium?

For drilling 0.8 mm holes in titanium, use speeds of 3000 to 10000 rpm depending on material hardness and desired chip clearance. Adjust feed rates from 20 to 80 mm/min as needed.

Why does my carbide drill get hot when drilling titanium?

Carbide drills get hot due to titanium's low thermal conductivity and high reactivity with coatings. Use coated tools like DC426L for better performance at temperatures up to \(93 \, \text{HRC}\).

What size hole can the DC426L drill make in titanium?

The DC426L series covers diameters from 0.04 mm to 3 mm. For drilling 0.8 mm holes in titanium, select a geometry value of 0.8 for optimal results and chip clearance.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index