Carbide tools with high thermal conductivity and hot-hard coatings resist titanium's heat retention better than other materials.
This allows maintaining cutting speeds that remove more material faster, reducing cycle times efficiently. Lowering speed too much can increase risk of work hardening near the surface.
AlTiN coating withstands higher temperatures compared to TiCN or TiAlN, preserving edge sharpness longer during machining.
Selecting a 135-degree point angle geometry ensures optimal chip evacuation and reduces thrust forces on the tool holder.
DC426L series offers diameters from 0.04 mm to 3 mm, suitable for precise drilling operations in titanium alloys.
The mechanism
Carbide's high hardness resists wear at the cutting edge during titanium drilling. This material maintains its strength even when heated by friction.
The AlTiN coating provides a barrier against chemical reactions with titanium at elevated temperatures. It remains effective up to 900 degrees Celsius, ensuring durability in challenging conditions.
A point angle of 135 degrees helps distribute forces evenly across the cutting edge. This design reduces stress concentration and enhances tool life during drilling operations.
Positive geometry minimizes cutting resistance by directing chips away from the workpiece efficiently. This feature allows for smoother chip formation and easier material removal.
Low cutting speeds combined with positive rake angles reduce heat generation at the cutting zone. Slower feeds allow more time to dissipate heat through the carbide before reaching the tool surface.
| Specification | Value |
|---|---|
| Point angle | 135 ° |
| Diameter | 1 mm |
| Carbide hardness | 89–93 HRC |
| Coating | AlTiN |
| Series diameter range | 0.04–3 mm |
The conditions that produce it
Carbide's thermal conductivity ranges from 80 W/(m·K) to 100 W/(m·K). This property helps dissipate heat away from the cutting edge during drilling.
A coating like AlTiN, with a hardness of HV3200 to HV3500 and a max temperature of 900 °C, resists titanium's chemical attacks at high temperatures.
The geometry's point angle of 135 degrees minimizes contact area with the workpiece, reducing heat generation. A smaller diameter tool reduces cutting forces.
Maintaining low cutting speeds between 40 m/min and 80 m/min keeps the temperature lower during drilling operations. Positive chip control improves heat removal from the cut zone.
Selecting a feed rate of 20 mm/min to 80 mm/min helps manage the chip thickness, ensuring effective cooling through increased chip formation.
How to recognise it on the tool
The carbide drill for titanium has a distinct chamfer that reduces edge chipping. This chamfer is usually ground with a blue dye visible under magnification.
Coating layers appear smooth and uniform across the flute surface; any irregularities indicate wear or damage. The AlTiN coating appears grayish-blue, often mistaken for an oxide film from cutting.
What actually removes the cause
AlTiN coating has high hardness and can withstand temperatures up to 900 °C. This allows it to resist titanium's chemical attack at elevated temperatures.
Drilling with a low cutting speed reduces heat accumulation at the edge, extending tool life. Positive rake geometry directs chips away from the cutting zone efficiently.
Carbide's thermal conductivity of 80 W/(m·K) to 100 W/(m·K) helps move heat into the workpiece and coolant rather than concentrating it at the edge.
A point angle of 135 degrees spreads forces over a larger area, reducing stress concentration and wear. This geometry supports lower cutting speeds for titanium drilling.
Coolant should be applied continuously to carry away generated heat quickly from the small contact area. This prevents overheating that could compromise tool integrity during prolonged use.
Frequently asked
How do I choose the right carbide drill for titanium?
Select a high-hardness carbide drill coated with AlTiN for better heat resistance up to \(900^\circ\)C. Use a point angle of \(135^\circ\) and maintain low speeds and positive feeds.
What is the right feed rate for drilling titanium with DC426L?
For DC426L drills, use a feed rate between \(20\) mm/min to \(80\) mm/min depending on material hardness. Higher feed rates remove more heat from the cutting zone faster, reducing tool wear.
Why does my carbide drill get hot when drilling titanium?
Titanium retains heat at the cutting edge due to low thermal conductivity. Use a coating like AlTiN that can handle high temperatures and reduce cutting speeds to manage heat effectively.