ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Selection guide: Drilling carbon-fibre reinforced polymer

CFRP is abrasive and layered: the fibres blunt the edge and the resin softens at heat. A sharp diamond-like or uncoated edge with a 130-degree point and peck...

4 min read 834 words Updated 2026-04-06
Carbon fibre composite panel edge with a drilled hole — Selection guide: Drilling carbon-fibre reinforced polymer

A sharp, diamond-like coated edge with a 130-degree point minimizes delamination when drilling carbon fibre reinforced polymer. This geometry and coating combination resists wear from abrasive fibres while maintaining precision cuts. A peck cycle reduces heat buildup, preventing resin softening that can lead to tool damage. Choosing the right feed rate is crucial; lower speeds extend tool life in hard materials. Higher feeds suit softer layers, ensuring efficient chip evacuation and surface finish quality.

The mechanism

Carbide's hardness resists wear from abrasive carbon fibres. Diamond-like coating stays sharp at high temperatures, preventing resin softening and edge blunting. Point angle of 130 degrees ensures minimal delamination when entering layered CFRP material. Sharp edges cut cleanly through fibre layers without excessive heat generation. Peck cycles remove chips regularly, cooling the drill tip.

Reduced feed rates help manage cutting temperature and prevent overheating issues. Supporting the exit side with gentle feeds prevents edge wear and prolongs tool life. Using uncoated tools at higher temperatures might be necessary if DLC coating fails. Adjust spindle speeds according to material thickness for optimal drilling performance. Lower rpm values reduce stress on the drill tip during deep-hole operations.

CoatingHardnessTop service temperature
DLC1800–2200 HV350–400 °C
uncoated1800–2000 HV700–800 °C

The conditions that produce it

Carbide's hardness range of 1800 to 2000 HV resists wear from abrasive carbon fibres in CFRP drilling. Diamond-like coating, with a hardness of 1800 to 2200 HV and max temperature up to 350–400 °C, maintains sharpness during cutting. Uncoated tools withstand higher temperatures up to 700–800 °C but require frequent resharpening due to heat-induced wear. A peck cycle with a feed rate of 50 mm/min at 25000 rpm prevents resin from softening and fibre breakage during entry. Reducing the feed rate to 75 mm/min and increasing spindle speed to 18000 rpm minimizes delamination on exit for cleaner holes.

A sharp, 130-degree point geometry ensures minimal material deformation upon entering CFRP layers. High cutting speeds of 100–180 m/min help manage temperature rise during drilling operations efficiently. Lowering the feed rate to 180 mm/min at reduced spindle speed of 15000 rpm prevents excessive heat build-up. Supporting the exit side rather than increasing feed helps maintain tool integrity and prolongs its service life. This approach ensures consistent performance across different CFRP materials and thicknesses during drilling operations.

How to recognise it on the tool

The uncoated carbide tool has a sharp edge and a 130-degree point angle, visible as a fine tip under magnification. When coated with diamond-like carbon (DLC), it appears darker than bare carbide but retains the same precise geometry. On parts, the hole edges show no signs of chipping or delamination if drilled correctly. Misalignment or excessive feed rate causes surface roughness and fibre tear.

Uncoated tools may appear similar to black oxide coated ones at first glance. Yet, under a microscope, uncoated carbide shows its true metallic shine without any coating residue. Confusion can arise with standard steel drills due to their comparable size but different performance in CFRP. Steel drills dull quickly and leave visible marks on the workpiece surface.

What actually removes the cause

The DLC coating's higher hardness range from 1800 to 2200 HV better resists wear compared to uncoated carbide’s 1800 to 2000 HV. This allows tools to maintain sharpness longer during drilling of carbon fibres and resin in CFRP. At temperatures up to 350 to 400 °C, the DLC coating remains intact, preventing edge blunting that occurs when uncoated carbide softens above 700 to 800 °C. Maintaining sharpness reduces fibre cutting forces and heat at the tool tip. A common misconception is increasing feed rate improves drilling speed in CFRP. However, this can cause excessive heat buildup and resin melting around the drill point.

Using peck cycles with controlled feeds prevents these issues. Uncoated carbide tools with a 130-degree point angle better manage entry and exit points in layered CFRP structures. This geometry minimizes delamination by providing gradual material engagement at both ends of the hole. Supporting the tool's exit side with adequate rigidity ensures consistent cutting forces, reducing edge wear and prolonging tool life during drilling operations. Proper support also helps maintain dimensional accuracy of holes drilled through multiple layers of CFRP.

Frequently asked

What coating should I use for drilling CFRP?

For carbon-fibre reinforced polymer, choose DLC coating due to its high hardness and heat resistance up to 350–400 °C, making it durable against wear and fibre abrasion.

How do I set the cutting speed when drilling CFRP?

Use a recommended rpm range of 25000 for small diameters down to 18000 or 15000 for larger sizes. Match feed rates according to tool diameter, ensuring optimal chip formation and heat management.

Why is a sharp point angle important in CFRP drilling?

A 130-degree point angle reduces entry force and minimises delamination at the start of cut, protecting the delicate layers from damage during drilling operations.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index