Drilling copper alloys requires a sharp, low-friction tool to prevent built-up edge and maintain cutting efficiency. The DC336 series with DLC coating excels in high-speed operations due to its reduced friction and superior wear resistance at elevated temperatures. This design minimizes chip adhesion on the cutting edge, ensuring cleaner holes and longer tool life during drilling tasks. Carbide hardness of 89–93 HRC combined with thermal conductivity up to 100 W/(m·K) supports rapid heat dissipation from the cutting zone. At temperatures reaching 400 °C, the DLC coating maintains its integrity and prevents material transfer between workpiece and tool.
The mechanism
Carbide's high hardness ranges from 89 to 93 HRC, making it extremely wear-resistant during drilling operations.
The thermal conductivity of carbide at 80 to 100 W/(m·K) helps dissipate heat generated by cutting.
| Coating | Hardness | Top service temperature |
|---|---|---|
| DLC | 1800–2200 HV | 350–400 °C |
| uncoated | 1800–2000 HV | 700–800 °C |
The conditions that produce it
The thermal conductivity of carbide ranges from 80 to 100 W/(m·K), helping dissipate heat during drilling operations. This property keeps the tool temperature lower than in copper alloys, reducing adhesion issues.
Using a DLC coating on DC326 and DC336 tools lowers friction between the cutting edge and workpiece surface. A sharp positive rake angle reduces thrust forces, enhancing chip control and preventing built-up edge formation. Select spindle speeds above 16000 rpm to maintain high surface finish quality and tool life. For optimal performance, apply a feed rate of 50 mm/min when drilling copper alloys with these tools. High-speed machining at 250 m/min minimizes heat buildup, further preventing built-up edge formation on the cutting edges.
How to recognise it on the tool
The DC336 series features a diamond-like carbon (DLC) coating visible as a smooth black layer on its surface. This coating has a hardness range between 1800 and 2200 HV, providing superior wear resistance at high temperatures up to 400 °C.
On the part, look for clean entry and exit surfaces without signs of built-up edge or excessive heat discoloration. The tool's sharp positive rake angle minimizes cutting forces and reduces friction against the workpiece material. Compare it with uncoated tools which may show more wear marks and a duller finish after drilling operations due to higher adhesion and friction levels.
What actually removes the cause
The DLC coating on DC336 tools reduces friction between copper chips and the tool surface. This low-friction layer prevents chip adhesion during drilling operations. A sharp positive rake angle further minimizes contact time with workpiece material. High spindle speeds enhance heat dissipation, keeping temperatures below bonding thresholds. These mechanisms together minimize built-up edge formation effectively.
A common alternative involves using uncoated tools or softer coatings like TiN. However, these options do not reduce friction as efficiently as DLC. Higher friction leads to increased adhesion and higher tool wear rates. Lower spindle speeds might decrease temperature but also increase cutting forces. This combination often results in more frequent stops due to built-up edge formation.
Frequently asked
What is the right drill for copper alloys?
For drilling copper alloys without built-up edge, use DC336 drills with a DLC coating and sharp positive rake geometry at high spindle speeds.
How do I prevent chip welding when drilling copper?
Use carbide drills like DC326 uncoated or DC336 with DLC coating. Maintain low point angles for reduced thrust and apply lubrication to minimise heat buildup and chip adhesion.
What are the optimal settings for drilling aluminium?
Optimal settings include high spindle speeds: 25000 rpm for small diameters, feed rates of 100 mm/min, and cutting speeds vc between 150-250 m/min.