A low-friction diamond-like carbon (DLC) coating reduces friction between the tool and workpiece, decreasing built-up edge formation during cutting. Built-up edges can occur due to adhesion at high temperatures or pressures, especially with soft materials like aluminium. This coating maintains a consistent performance even when operating within its temperature limits of 350 to 400 degrees Celsius, ensuring minimal friction-related issues for the tool. Lower friction means less likelihood of chip welding on the rake face, enhancing tool durability and surface finish quality during machining operations.
What the coating does in this cut
A low-friction DLC coating on DC336 tools minimizes friction at the tool-work interface during cutting processes. This reduces adhesion between the chip and rake face, decreasing built-up edge formation. However, a sharp cutting edge is essential to prevent wear before adhesion occurs. Maintaining optimal cutting speeds also prevents excessive heat buildup that can weaken the coating.
Stainless steel requires lower feed rates compared to aluminium to minimize friction and maintain tool life. DLC coatings work right with proper chip control strategies such as using adequate coolant or selecting appropriate geometry for material type. Coatings enhance performance but cannot compensate for dull edges or incorrect machining parameters. Regular inspection of cutting tools ensures efficient operations and prolongs tool lifespan.
| Coating | Hardness | Top service temperature |
|---|---|---|
| DLC | 1800–2200 HV | 350–400 °C |
| TiN | 2400–2500 HV | 550–600 °C |
| uncoated | 1800–2000 HV | 700–800 °C |
The chemistry between coating and workpiece
The DLC coating on DC336 tools has a hardness range of 1800 to 2200 HV, making it resistant to wear at high temperatures up to 400 °C. This temperature range is critical because it matches common cutting scenarios for both aluminium and stainless steel. At these conditions, the DLC coating reduces friction significantly compared to TiN or uncoated tools. TiN coatings offer higher hardness from 2400 to 2500 HV but start degrading above 600 °C.
They provide better wear resistance than DLC under certain conditions but have higher friction against common metals. Uncoated carbide has the highest thermal stability, remaining effective up to 800 °C. However, its surface can suffer from increased adhesion and built-up edge formation when cutting softer materials like aluminium at high speeds.
How it fails
DLC coating failure typically starts with reduced lubricity at high temperatures, causing increased friction. This elevated friction can lead to adhesion between chip and rake face despite DLC's low-friction properties. Adhesion leads to built-up edge formation if cutting speed is too low or tool sharpness insufficient. Proper geometry and optimal cutting parameters prevent this issue regardless of coating type. Substrate wear occurs when the carbide core degrades due to high temperatures, not from adhesion issues. Once DLC fails, underlying carbide experiences increased contact stresses at elevated temperatures.
Without DLC protection, the carbide substrate wears faster above 400 °C. This temperature range accelerates wear mechanisms like oxidation and diffusion. Regular inspection is necessary to catch early signs of wear before damage spreads. Coating failure also affects tool lifespan indirectly by compromising overall performance. Once adhesion occurs, machining efficiency drops as forces increase. Proper maintenance and monitoring extend tool life beyond initial failures.
Choosing between the available options
For DC336 tools, selecting a coating depends on operating temperatures and material being cut. DLC coatings resist high friction at up to 400 °C for aluminium cutting. DLC’s lower temperature range prevents adhesion issues but limits its use for higher-temperature stainless steel work. TiN operates safely up to 600 °C, ideal for both materials. Uncoated carbide offers the highest service temperature of 800 °C but wears faster without a protective layer.
Choose TiN over DLC if machining temperatures exceed 400 °C. Lower cutting speeds and dull edges increase adhesion risk more than coating choice does. Ensure optimal speeds to prevent built-up edge formation regardless of tool coating. Stainless steel requires slower cutting speeds compared to aluminium, affecting the choice between DLC and TiN coatings for durability and temperature resistance.
Frequently asked
What is built-up edge on carbide tools?
Built-up edge is chip adhesion, not wear. Low-friction coatings like DLC can reduce this by preventing chips from welding to the tool's rake face, but sharp edges and correct cutting speeds are crucial.
How does coating hardness affect performance in high-temperature applications?
Harder coatings like TiN (HV 2400–2500) resist wear better than softer ones like DLC (HV 1800–2200). However, DLC can operate at lower temperatures ([350, 400] °C), making it suitable for applications prone to galling.
Why do I need a sharp edge when using coated tools?
A dull edge increases friction and heat, promoting chip welding. Even with coatings like TiN or DLC, maintaining sharpness ensures smooth cutting without built-up edges.