ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Drilling 0.05 mm holes in engineering plastic

At 0.05 mm the tool is slender enough that any side load bends it before the edge dulls, so the whole process is about keeping the load axial. Plastics melt...

4 min read 780 words Updated 2026-04-05
Machined engineering plastic component with clean drilled holes — Drilling 0.05 mm holes in engineering plastic

DC326L carbide drills ensure axial cutting for 0.05 mm holes in engineering plastics. Hardness ranges from 89 to 93 HRC, maintaining durability under high friction. RPM settings vary between 25,000 and 15,000 to control heat generation. Feed rates range from 50 to 750 mm/min for optimal plastic melting without overheating. This precision minimizes hole distortion, ensuring consistent quality in micro-drilling operations.

The physics at this diameter

At 0.05 mm, the drill's slender form requires precise axial alignment to prevent bending from side loads. Side loads cause premature wear or breakage due to the tool’s thinness. Plastics melt at temperatures far below metal cutting limits; frictional heat and material softening dictate process parameters. High rotational speeds around 25000 rpm help maintain a stable temperature below plastic's melting point.

Friction generates excessive heat when feed rates exceed optimal values, causing material to soften prematurely. Optimal feed rates range from 50 mm/min for precise drilling to 750 mm/min for faster operations. The hole diameter closes due to material softening if cutting speeds drop or side loads rise. Proper geometry and coating reduce friction, ensuring consistent hole quality in plastics.

SpecificationValue
Diameter0.05 mm
Carbide hardness89–93 HRC
Series diameter range0.04–3.01 mm

What this material demands

At 0.05 mm diameter, the drill cuts plastic that melts from frictional heat, not metal cutting temperatures. This melting can cause material to adhere to the tool edge, increasing friction and wear. To prevent this, maintain a high rotational speed of 25000 rpm or above for optimal chip formation and evacuation. Slower speeds can lead to excessive heat buildup, causing plastic deformation around the hole. Choose feeds between 50 mm/min and 75 mm/min to balance cutting efficiency with tool life. At higher cutting data, like 180 m/min in velocity, the drill experiences less friction because of faster chip removal.

Lower velocities increase contact time, raising heat issues. Maintaining axial alignment is crucial at all times to avoid bending or breakage due to side loads. Plastic deformation behind the tool limits hole quality if temperatures rise too high. This issue can be mitigated by selecting the appropriate cutting parameters as per the provided data range. Proper selection ensures that friction remains below plastic softening point, maintaining dimensional accuracy and surface finish.

Tooling that fits the combination

For 0.05 mm diameter holes, DC326L carbide drills with a hardness range of 89 to 93 HRC are crucial for axial cutting in engineering plastics. These drills prevent bending due to side loads by maintaining precise alignment and reducing wear or breakage risks. Side loads can lead to early tool failure. The drill geometry minimizes contact area, decreasing frictional heat that could soften plastic material. Softened material tends to adhere to the tool surface, degrading performance.

A TiAlN coating on DC326L enhances lubricity and reduces temperature rise during cutting operations. This coating prevents plastic from sticking to the tool edge. High hardness ensures wear resistance in thin cross-sections, preserving sharpness needed for clean holes. Reduced friction also minimizes heat buildup, crucial for maintaining hole quality.

Cutting data and where it stops working

When drilling with a 0.05 mm diameter tool, increasing feed rate first causes plastic deformation rather than cutting chip formation. As feed increases beyond optimal limits, frictional heat rises sharply, softening the material. Softened plastic can squeeze back into the hole as the drill exits, closing it partially or completely. This effect becomes more pronounced at higher speeds and feeds due to increased friction and heat generation.

RPM reduction alone does not prevent this issue; maintaining axial alignment and optimal feed rate is crucial for preventing deformation and maintaining hole quality. Exceeding recommended parameters risks overheating the plastic, which leads to adhesion on the tool surface. At lower RPMs but high feed rates, the tool may experience excessive side loads and bending forces, compromising its structural integrity. Monitoring these variables ensures consistent drilling performance in engineering plastics without causing premature wear or breakage.

Frequently asked

What is the recommended rpm for drilling 0.05 mm holes?

Use speeds of \(25\,000\) rpm for carbon plastics. For nylon and other materials, reduce to \(18\,000\) or \(15\,000\) rpm based on material hardness.

How do I avoid melting the plastic when drilling small holes?

Maintain low axial loads and high speeds to keep heat below the softening point of plastics. Use feeds like \(75\) mm/min for optimal results without overheating.

What is the right carbide tool for 0.05 mm diameter drills?

Use DC326L series with uncoated options, suitable for diameters from \(0.04\) to \(3.01\) mm. This ensures durability and precision at small sizes.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index