ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Edge deformation in hardened steel

The edge deforms plastically under the high specific force before it wears out, so the corner rounds and the hole loses size. A stronger edge preparation, no...

4 min read 780 words Updated 2026-10-21
Tight coil of steel swarf on a machine table next to a drilled plate — Edge deformation in hardened steel

A harder carbide edge reduces plastic deformation when cutting hardened steel, maintaining hole size accuracy. Carbide hardness between 89 and 93 HRC ensures durability against high forces during machining. This resilience minimizes corner rounding at various cutting speeds and feeds, from 70 to 130 m/min. The DC836 series with a 140-degree point angle provides consistent performance across different materials. By selecting the right edge preparation, users can achieve precise hole sizes without frequent adjustments.

The mechanism

High hardness of carbide edges reduces plastic deformation when cutting hardened steel, maintaining hole size accuracy. Deformation happens before wear under high specific force. Carbide with hardness between 89 and 93 HRC resists plastic deformation better than softer options. This keeps corners sharp during the initial stages of cutting operations. A point angle of 140 degrees on these tools balances strength and chip clearance.

Proper feed rates, like 40 to 60 mm/min, prevent excessive force buildup at the cutting edge. Reducing feed to 270 mm/min for softer materials avoids overloading the tool tip. Lower speeds such as 9000 rpm also reduce stress concentration on the edge. Using these parameters ensures minimal deformation during machining of hardened steel parts. Hole size accuracy remains consistent throughout the operation, improving overall part quality.

SpecificationValue
Point angle140 °
Carbide hardness89–93 HRC
Series diameter range0.1–14 mm

The conditions that produce it

High hardness of carbide edges reduces plastic deformation when cutting hardened steel, maintaining hole size accuracy. Deformation happens before wear starts. Plastic deformation occurs at higher cutting speeds and feeds, such as 70 to 130 m/min and 40 to 270 mm/min. Lower speeds and feeds reduce the risk of deformation. Deformation also increases with larger chip thicknesses, typically found in roughing operations compared to finishing.

Smaller chip thicknesses during finish machining minimize plastic flow at the edge. Choosing a stronger geometry, like point angles below 140 degrees, further resists deformation. Stronger geometries distribute forces more evenly across the cutting edge and flank face. Carbide hardness between 89 and 93 HRC provides optimal resistance against plastic deformation in hardened steel applications. This range of hardness ensures better dimensional stability during machining.

How to recognise it on the tool

On a carbide cutting tool, edge deformation in hardened steel appears as rounded corners instead of sharp edges. This rounding is more noticeable on parts with smaller diameter holes. The corner radius increases as the deformation progresses.

Operators may confuse this condition with normal wear because both cause larger hole sizes than intended. However, plastic deformation leaves marks that look different from typical wear patterns. Deformed areas show a smoother surface compared to worn-out surfaces which are typically rougher. To prevent excessive rounding, use stronger edge preparations like chamfers or relief angles during tool design. Adjusting the cutting parameters can also help maintain sharpness and reduce deformation risks.

What actually removes the cause

A stronger edge preparation reduces plastic deformation in hardened steel by increasing resistance at the cutting edge. This allows the tool to maintain its shape under high specific forces. Using a sharper point angle does not address the root cause of deformation effectively. It may initially improve surface finish but leads to rapid wear and reduced durability. The geometry with 140-degree point angles offers better stability against plastic flow during cutting operations.

Higher edge strength means less rounding even at extreme feeds and speeds listed. Common practice often involves decreasing the point angle for finer cuts, which actually weakens the edge under severe conditions. This results in faster degradation of tool accuracy over time. Edge deformation is mitigated not by sharpness alone but through design features that enhance structural integrity. DC836 tools use robust geometries proven to resist plastic deformation during tough machining tasks.

Frequently asked

Why does my carbide drill edge deform when cutting hardened steel?

Edge deformation happens due to plastic deformation under high specific force before wear occurs, which leads to rounded corners and inaccurate holes. Use a stronger edge preparation rather than a sharper one for better performance.

What is the right rpm range for DC836 drills in hardened steel?

For optimal performance of DC836 drills in hardened steel, use an rpm range of 20000 down to 9000 depending on material hardness and required cutting speed (vc) between 70 and 130 m/min.

How do I prevent corner rounding when drilling with carbide tools?

To avoid corner rounding during drilling in hardened steel, select a geometry that provides stronger edge preparation rather than an overly sharp one. Opt for point angles like 140° and appropriate coating types such as bronze.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index