ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Sensor housing and thin-wall parts

Thin-wall housings deflect under thrust, so the hole is made by a tool that pushes lightly rather than by a fixture that holds harder. A blunt point makes th...

5 min read 938 words Updated 2026-05-05
A micro drill entering a clamped metal block on a machine table — Sensor housing and thin-wall parts

DC326 tools feature an 118-degree point angle and uncoated carbide, ideal for thin-wall parts where deflection is critical. Carbide hardness ranges from 89 to 93 HRC, ensuring durability during light cutting required in thin walls. Feed rates of 50 mm/min to 1200 mm/min and spindle speeds up to 25000 rpm suit various machining conditions. Thin-wall applications benefit from precise control over axial depth, reducing the risk of deformation or breakage at critical points. This geometry minimizes thrust force while maintaining cutting efficiency for consistent surface finishes on sensor housings.

The process requirement

Carbide hardness from 89 to 93 HRC ensures wear resistance during machining thin-wall parts under light cutting forces. An 118-degree point angle reduces thrust at the thinnest part of walls, minimizing deflection compared to sharper tools. Cutting data varies with material: aluminium requires speeds from 25000 rpm down to 16000 rpm for optimal performance. Feed rates range between 50 mm/min and 1200 mm/min depending on the specific cutting conditions and tool diameter. The DC326 series operates efficiently within a diameter range of 0.04 mm to 3.17 mm, accommodating diverse part requirements.

Chip thinning compensation is critical for maintaining surface finish and dimensional accuracy during machining operations. Negative radial rake angles help control chip thickness and manage cutting forces effectively in thin-wall applications. Minimum clearance ensures chips evacuate cleanly without causing built-up edge or increased friction against the workpiece. The uncoated carbide reduces heat generation, extending tool life under continuous light-pressure conditions typical for sensor housings.

SpecificationValue
Point angle118 °
Carbide hardness89–93 HRC
Series diameter range0.04–3.17 mm

What it demands of the tool

Carbide hardness from 89 to 93 HRC provides wear resistance for thin-wall parts under light cutting forces. This range ensures durability during machining with minimal damage. An 118-degree point angle reduces stress concentration at the thinnest part of walls, preventing deflection and breakage. Lighter cuts, like those at 50 mm/min feed rate, minimize force on sensitive areas. At higher speeds such as 250 m/min, the tool maintains stability despite reduced rigidity in thin-wall sections.

Tool geometry must balance wear resistance with cutting efficiency for optimal performance. Lower spindle speeds of 16000 rpm allow more precise control over cut depth and feed rates. This ensures consistent material removal without excessive stress on the workpiece. Uncoated carbide minimizes friction between the tool and workpiece, reducing heat generation during machining operations. This feature supports longer tool life in thin-wall applications where cooling is challenging.

Where it usually goes wrong

The most common failure occurs when the point angle is too sharp, increasing stress concentration at the thinnest wall part. A sharper angle concentrates force, causing premature wear and potentially breaking the tool. Using an 118-degree point reduces this risk by spreading out the contact area more evenly. Lower cutting forces allow the thin walls to maintain their shape better during machining operations. Higher hardness from 89 to 93 HRC supports durability without needing excessive clamping pressure.

Choosing incorrect speeds and feeds can also lead to overheating, accelerating wear on carbide tools. Aluminium requires specific rpm settings: 25000 for thin walls down to 16000 for thicker sections. Appropriate feed rates range from 50 mm/min to 1200 mm/min based on wall thickness and hardness. Maintaining a constant surface speed between 150 and 250 m/min is crucial for optimal tool life. Adjusting these parameters correctly ensures consistent cutting performance in thin-wall applications.

Setting up for it

To prevent excessive stress at the thinnest part of the housing, use a tool with an 118-degree point angle for better stability under light cutting forces. Start by selecting DC326 carbide tools with hardness between 89 and 93 HRC for optimal wear resistance during machining operations on thin walls. Adjust spindle speed according to material type: set it at 25000 rpm for aluminium, reducing gradually to 16000 rpm as necessary for other materials. Feed rate should be kept moderate; start with 50 mm/min and increase cautiously to avoid deflection in the thin walls of sensor housings during cutting operations. Ensure cutting speed stays within the range of 150 to 250 m/min to balance efficiency and tool life, preventing premature wear or failure under light machining conditions.

For precise control over wall thickness without compromising structural integrity, maintain feed rates at lower values like 100 mm/min for more delicate operations. Reduce spindle speed incrementally if the thin walls begin to deflect; this helps minimize cutting forces and prevents damage during the final stages of part production. Select a higher cutting speed of up to 250 m/min initially when starting work on thicker sections, then adjust downwards as walls become thinner near completion. Use feed rates between 1000 mm/min and 1200 mm/min for larger areas where structural support is better, ensuring consistent material removal throughout the process. Monitor tool wear closely by inspecting regularly to maintain optimal cutting conditions and prolong tool life during machining of thin-wall sensor housing parts.

Frequently asked

How do I prevent deflection when making thin-wall parts?

Use tools that apply light pressure, such as the DC326 series carbide cutter. Avoid sharp points which can worsen deformation at the thinnest part of the wall.

What is the point angle for the DC326 tool?

The DC326 tool uses an 118° point angle, suitable for thin-wall applications where deflection must be minimised.

What are the recommended cutting speeds and feeds for aluminium with DC326 tools?

For aluminium, use DC326 at speeds of 150 to 250 m/min and feed rates from 50 to 1200 mm/min depending on the tool diameter.