DC336 drills pultruded glass fibre profiles with minimal splitting thanks to its sharp edge and supported exit design. This geometry prevents fibres from tearing at entry, ensuring smoother holes. The tool's hardness range of 89–93 HRC maintains durability for repeated drilling cycles. Supported exit reduces stress on exiting cut edges, further preventing splits along the fibre direction. This results in cleaner holes that require less post-processing and meet quality standards more reliably.
The process requirement
The process requires a hole with consistent diameter across the profile, avoiding fibre splitting and reducing material waste. Splitting occurs along unidirectional fibres because they resist cutting forces more than resin. A sharp edge geometry minimizes entry force, allowing for smoother drilling operations. The supported exit design ensures continuous material removal without damaging exiting fibres. Recommended spindle speeds range from 25000 rpm down to 15000 rpm based on fibre orientation and tool diameter.
Feeds vary between 50 mm/min in delicate applications up to 750 mm/min for robust drilling conditions. Coating durability supports the sharp edge during extended operation, maintaining hole quality over time. A hardness range of 89–93 HRC ensures long-lasting performance under high-pressure cutting scenarios. This geometry effectively handles resin-rich areas while preventing fibre breakage at entry and exit points.
| Specification | Value |
|---|---|
| Point angle | 130 ° |
| Carbide hardness | 89–93 HRC |
| Series diameter range | 0.07–4.98 mm |
What it demands of the tool
A sharp cutting edge is crucial for DC336 because pultruded glass fibre profiles contain aligned fibres that can cause splitting if the tool lacks precision.
The hardness of DC336 ranges from 89 to 93 HRC, ensuring durability against wear and tear during drilling operations at high speeds and feeds.
Where it usually goes wrong
The most common failure occurs when the drill exits the material after encountering aligned fibres. These fibres can cause premature wear on the cutting edge if unsupported. Wear reduces the sharpness of DC336’s geometry over time, allowing for fibre splitting along the exit point. Splitting increases as fibres encounter a duller tool angle and unsupported exit design weakens. Proper coolant application during drilling is crucial to extend tool life by reducing wear.
Insufficient cooling leads to rapid edge deterioration and increased risk of profile damage. Adjusting cutting parameters can help mitigate wear issues, such as decreasing feed rates or increasing spindle speeds. These adjustments reduce the stress on the drill’s cutting edge but require precise control. Operators should monitor the sharpness of DC336 regularly during drilling operations. Replacing dull tools prevents excessive fibre splitting and maintains hole quality throughout the process.
Setting up for it
Set up the DC336 with a 130-degree point angle for optimal entry into pultruded glass fibre profiles. Use recommended spindle speeds: 25000 rpm for softer areas, 18000 rpm for harder zones, and 15000 rpm in transitional regions.
Apply feed rates of 50 mm/min for initial engagement, increase to 75 mm/min within the profile, then boost to 180 mm/min near exit. Ensure constant surface speed between 100 m/min and 180 m/min throughout operation.
Frequently asked
What is the right rpm for drilling pultruded glass fibre profiles?
Use 25000 rpm for smaller diameters, reduce to 18000 rpm and 15000 rpm as diameter increases up to 4.98 mm. Ensure sharp edge and supported exit on carbide tool.
What feed rate should I use with DC336 for pultruded fibre profiles?
Apply a slower feed of 50 mm/min initially, then adjust to 75 mm/min or higher depending on material thickness and machine capacity. Higher speeds up to 750 mm/min work well for thinner sections.
How do I prevent splitting when drilling glass fibre profiles?
Use DC336 with an angle of 130 degrees. Maintain sharp edges and ensure the tool has a supported exit after cutting through fibres to avoid splitting along their length.