At high speeds, cobalt binder softens before carbide grains wear out, causing edge deformation and size loss in holes. This softening leads to rounded corners rather than chipped ones, affecting hole quality. The DC836 series, with a hardness range of 89–93 HRC, operates optimally at speeds up to 130 m/min without binder issues. Below this speed, the tool maintains its geometry and performs well in various applications. Manufacturers can achieve precise holes by selecting appropriate cutting parameters within the given rpm and feed ranges.
The mechanism
At high speeds, the cobalt binder softens before carbide grains wear out. Cobalt's lower melting point causes it to deform under pressure and heat. This deformation changes the cutting edge geometry, making holes larger than intended. As a result, the tool’s corner becomes rounded rather than chipped. The softened edge cannot maintain its sharpness during high-speed operations.
The 89–93 HRC hardness of carbide grains ensures durability against wear at lower speeds. However, above certain thresholds, cobalt binder softens first due to increased temperature and mechanical stress. This softening occurs even before visible signs of wear appear on the cutting edge. The softened cobalt allows for plastic deformation, affecting hole diameter accuracy significantly. Thus, maintaining optimal speed prevents premature tool deformation and size loss in machined holes.
| Specification | Value |
|---|---|
| Point angle | 135 ° |
| Carbide hardness | 89–93 HRC |
| Series diameter range | 0.1–14 mm |
The conditions that produce it
Substrate softening occurs when cutting speeds exceed 70 m/min for DC836 alloy steel tools. At these high speeds, cobalt binder begins to soften before carbide grains wear out significantly. This deformation causes the tool’s edges to round and lose their sharpness quickly. The softened substrate leads to plastic deformation rather than brittle fracture of the cutting edge. To avoid this issue, reduce feed rates below 40 mm/min when using higher rpm settings.
For lower cutting speeds between 70 m/min and 89 m/min, soften the alloy gradually without causing severe edge rounding. This range allows for a balance between efficiency and durability. Decreasing speed to less than 70 m/min prevents substrate softening entirely. At these slower speeds, feed rates can be increased up to 100 mm/min safely. Using proper cutting parameters ensures consistent hole size and maintains tool life effectively.
How to recognise it on the tool
On a DC836 tool, substrate softening leaves rounded corners instead of sharp ones. This rounding happens when speeds exceed 70 m/min for alloy steel. The edge loses its sharpness due to plastic deformation rather than chipping or wear. On the workpiece, this appears as oversized holes with smoother edges compared to intended dimensions. Operators often confuse it with poor tool positioning or inaccurate machine settings.
Inspecting the DC836 under a microscope shows a polished surface at the cutting edge where softening occurs. The lack of sharpness indicates that cobalt has yielded before wear happened to carbide grains. At 135° point angles, softened edges become more visible as they round off faster than harder ones. This rounding is distinct from typical chipping patterns seen in lower-speed operations. Identifying this requires checking both the tool's condition and machining parameters for signs of overheating or excessive speed.
What actually removes the cause
Reducing cutting speed decreases substrate softening but limits productivity. Slower speeds allow cobalt binder to remain rigid during machining, preventing plastic deformation. However, this approach reduces material removal rate significantly, affecting shop efficiency negatively. An alternative is using a harder grade with higher cobalt content, improving wear resistance slightly. Yet, this solution does not address the fundamental thermal and mechanical issues at high speed.
A better fix involves selecting a geometry that distributes cutting forces more evenly across the tool edge. A 135-degree point angle helps in dissipating heat away from critical areas, reducing localized binder softening. This specific geometry also provides enhanced stability for higher feed rates without sacrificing precision. By choosing the DC836 grade with optimal geometry, users can maintain high production levels while minimizing substrate deformation risks. Combining these factors ensures consistent hole size and quality throughout machining operations.
Frequently asked
Why does my carbide drill get rounded corners instead of chipped ones?
At high speeds, cobalt binder softens before wear occurs on carbide grains, causing plastic deformation and loss of hole size precision. Check your cutting speed; above 70 m/min can cause this issue.
What is the hardness range for carbide tools used in alloy steel drilling?
Carbide tools used for alloy steel have a hardness range from 89 to 93 HRC, providing excellent wear resistance and durability during machining operations.
Can you recommend a specific drill geometry for alloy steel workpieces?
For alloy steel, use drills with a 135° point angle. This geometry helps in maintaining cutting edge sharpness and reduces the risk of tool deformation at high speeds.