ISO 9001 CERTIFIED MANUFACTURER IN-HOUSE GRINDING · COATING · INSPECTION

Drilling 0.2 mm holes in aluminium

At 0.20 mm the flute just has room to carry a chip, which makes evacuation possible for the first time in the micro range. Aluminium is soft, conductive and...

4 min read 860 words Updated 2026-06-26
Bright aluminium chips clustered around a freshly drilled hole — Drilling 0.2 mm holes in aluminium

DC326 drills 0.2 mm holes efficiently, thanks to its uncoated carbide hardness range from 89 to 93 HRC. This hardness prevents aluminium from welding to the tool edge, reducing wear and improving durability. The geometry is optimized for chip evacuation at these small diameters, ensuring consistent hole quality in soft materials. At speeds up to 250 m/min and feeds of 100 mm/min, DC326 maintains sharpness and performance over extended use. This makes it ideal for high-precision applications where reliability and accuracy are critical.

The physics at this diameter

At 0.3 mm diameter, chip evacuation through the flute is straightforward due to ample space for chip removal. At 0.2 mm, the flute narrows significantly, limiting chip clearance but enabling effective cutting. Material adhesion becomes critical at this size because a smaller flute means less volume for chip storage and more surface area for aluminium to bond with carbide edges. DC326's hardness range ensures minimal wear from high-speed cutting in aluminium. Tool geometry must precisely manage chip thickness to prevent blockage, necessitating careful feed rate selection.

Aluminium's thermal conductivity allows rapid heat dissipation, reducing the likelihood of carbide softening under friction. However, this property also encourages metal-to-metal bonding at microscopic levels if surfaces are not smooth enough. At 0.2 mm diameter, maintaining sharp edges through consistent tool use and correct cutting parameters is crucial for long-term performance. The reduced flute size requires lower feed rates compared to larger diameters, ensuring chips do not jam inside the drill's flutes during operation. A balanced approach between speed and pressure ensures efficient material removal without compromising edge integrity or chip flow dynamics.

SpecificationValue
Diameter0.3 mm
Diameter0.2 mm
Carbide hardness89–93 HRC
Series diameter range0.04–3.17 mm

What this material demands

At 0.2 mm diameter, chip evacuation is more challenging due to the narrow flute space available. This makes proper chip control essential for maintaining efficiency. Aluminium's tendency to weld to a sharp edge limits tool life, requiring frequent replacements or resharpening. Wear from cutting at high speeds up to 250 m/min is minimal compared to adhesion issues.

Adhesion can cause micro-chipping on the cutting edge and reduces drilling accuracy over time. Lower feed rates of 50 mm/min help mitigate this problem by reducing contact duration between aluminium and carbide. Higher feed rates, such as 1000 mm/min for larger diameters, allow chips to exit faster but increase adhesion risk at smaller sizes like 0.2 mm. Maintaining optimal cutting parameters ensures efficient drilling operations in micro ranges.

Tooling that fits the combination

DC326 uses an uncoated carbide core for optimal wear resistance and minimal aluminium welding. This coating-free design reduces edge buildup, enhancing tool life significantly. For 0.2 mm drills, a TiAlN coated version might seem suitable but adds friction and heat. Increased temperature softens the alloy prematurely, degrading performance quickly. Instead, DC326’s sharp geometry excels by maintaining consistent cutting forces throughout.

At lower diameters, chip control becomes critical due to reduced flute volume. A smaller flute traps chips, increasing risk of re-cutting or breakage. With proper feed rates and speeds, uncoated 89–93 HRC material stays sharper longer. Higher coating temperatures can cause premature dulling, reducing overall efficiency. DC326’s precise geometry minimises chip recutting issues effectively in micro-drilling operations.

Cutting data and where it stops working

At 0.2 mm diameter, drilling parameters start to shift as chip evacuation becomes critical. Higher spindle speeds typically move first when cutting fails, reducing to around 16000 rpm for stability. Feed rates also decrease significantly at these settings, dropping below 50 mm/min to prevent excessive pressure and heat buildup. Varying the depth of cut does not extend tool life as much as altering speed or feed rate. As vc drops from 250 m/min to 150 m/min, cutting efficiency diminishes due to reduced metal removal rates.

The material's thermal properties mean that adhesion rather than wear limits cutting duration at smaller sizes. The process limit occurs when the chip cannot be evacuated properly and starts to jam or wrap around the tool. This causes excessive heat buildup, which leads to rapid wear and potential breakage of the tool. Proper cooling is crucial but often challenging in such tight confines; insufficient coolant can exacerbate adhesion issues even further, pushing the practical limits closer together for smaller diameters.

Frequently asked

How do I drill aluminum with 0.2 mm bits?

Use carbide drills like DC326, designed for micro-drilling. Adjust cutting speed (vc) between 150 and 250 m/min and use feed rates from 50 to 1200 mm/min depending on your spindle rpm.

What is the right RPM range for drilling aluminum with a 0.3 mm drill?

For optimal results in aluminium, set your RPM at 25000 for small holes up to around 16000 for larger sizes using DC326 drills. Ensure feed rates match accordingly for efficient chip evacuation.

Why does the DC326 carbide drill have a flute size just big enough?

The design allows chips from drilling aluminium to be evacuated effectively, preventing clogging and improving tool life at high speeds due to its precise fit with material properties.

Data behind the text

Dimensions and part numbers referenced here come from the TONNY production catalogue. Open the series or diameter index to check a specific record before ordering.

Browse series   Diameter index